info:eu-repo/semantics/article
Influence of the Ir content and the support on the thiotolerance of the Ir/SiO2-Al2O3 catalysts for selective ring opening of decalin
Fecha
2021-05Registro en:
D'ippolito, Silvana Andrea; Ballarini, Adriana Daniela; Rosas, Santiago Miguel; Pirault Roy, Laurence; Especel, Catherine; et al.; Influence of the Ir content and the support on the thiotolerance of the Ir/SiO2-Al2O3 catalysts for selective ring opening of decalin; John Wiley & Sons Inc; The Canadian Journal Of Chemical Engineering; 99; 5; 5-2021; 1146-1157
0008-4034
CONICET Digital
CONICET
Autor
D'ippolito, Silvana Andrea
Ballarini, Adriana Daniela
Rosas, Santiago Miguel
Pirault Roy, Laurence
Especel, Catherine
Epron, Florence
Pieck, Carlos Luis
Resumen
The influence of Ir content on sulphur tolerance for the selective ring opening of decalin was investigated. Ir/SiO2-Al2O3 catalysts (70 wt% and 80 wt% SiO2) were used. In the absence of sulphur, slight differences were observed on the yields according to the metallic content regardless of the support used. Although the results of cyclopentane hydrogenolysis showed that the metallic function acquires importance as the metal content increases, for these metal percentages the acid function limits the rate of decalin opening reaction. Products distribution are strongly modified using decalin with S content compared to pure decalin. The formation of dehydrogenated products is virtually null due to S adsorbed on the metal sites. The support has low influence on the thiotolerance. The results, related to the amount of S per Ir surface atom, showed that for a moderate S content (S/Irsurf ∼ 0.30), 1.5 Ir/Sy appears to be less poisoned than 1Ir/Sy and 2Ir/Sy.