Processing, structural, and biological evaluations of zirconia scaffolds coated by fluorapatite
(Wiley Blackwell Publishing, Inc, 2018-11)
Highly porous zirconia (ZrO2) scaffolds fabricated by the replication method were coated with fluorapatite (FA). The FA coating was obtained by dipping the ZrO2 scaffolds into stabilized aqueous FA slips having different ...
Comparison of different fluorapatite dip coated layers on porous zirconia tapes
(Elsevier, 2014-09)
Fluorapatite (FA) layers with different thickness and microstructures on porous 3 mol% yttria-partially stabilized zirconia (Y-PSZ) substrates have been fabricated by dipping porous zirconia tapes into aqueous fluorapatite ...
Effect of zirconia tape porosity on fluorapatite surface film formation by dip coating
(Elsevier, 2013-01)
Thin fluorapatite (FA) layers on porous 3 mol% yttria-partially stabilized zirconia (Y-PSZ) substrates have been fabricated by dipping porous zirconia tapes into aqueous 27.4 vol% fluorapatite slurries. Two porous Y-PSZ ...
Comparison of two bond strength testing methodologies for bilayered all-ceramics
(Elsevier B.V., 2007-05-01)
Objectives. This study compared the shear bond strength (SBS) and microtensile (MTBS) testing methodologies for core and veneering ceramics in four types of all-ceramic systems.Methods. Four different ceramic veneer/core ...
Comparison of two bond strength testing methodologies for bilayered all-ceramics
(Elsevier B.V., 2007-05-01)
Objectives. This study compared the shear bond strength (SBS) and microtensile (MTBS) testing methodologies for core and veneering ceramics in four types of all-ceramic systems.Methods. Four different ceramic veneer/core ...
Comparison of two bond strength testing methodologies for bilayered all-ceramics
(Elsevier B.V., 2014)
Improved zircon fission-track annealing model based on reevaluation of annealing data
(SpringerNew YorkEUA, 2013)
Surface roughness analysis of dental ceramics treated with hydrofl uoric acid and aluminum oxide jet
(2014)
The aim of this study was to evaluate the surface roughness of 5 indirect restorative materials treated with hydrofluoric acid to 10%, with aluminum oxide jet and a combination of both. The specimens was prepared with 10 ...
Influence Of Different Adhesive Protocols On Ceramic Bond Strength And Degree Of Conversion Of Resin Cements
(ELSEVIER SCI LTDOXFORD, 2015)