Effects of the atmosphere and substrate on the crystallization of PLZT thin films
(ABM, ABC, ABPol, 2000-07)
Lead lanthanum zirconate titanate [PLZT (9/65/35)] thin films were prepared by dip-coating on Si (100) or Si/Ti/Pt (100) substrates using a polymeric precursor solution and annealed at 650 °C for 3 h. Perovskite phase ...
Influence of substrate temperature on formation of an SiC buffer layer by reaction of Si(100) with silane-methane plasma
(Iop Publishing LtdBristolInglaterra, 2000)
Magnetocoupling and domain structure of BiFeO3/ LaFeO3 heterostructures deposited on LaSrCoO3/Pt/TiO2/SiO2/Si (100) substrates by the soft chemical method
(2017-06-01)
BiFeO3 (BFO) and LaFeO3 (LFO) heterostructures were obtained at room temperature on Pt/TiO2/SiO2/Si (100) substrates by chemical solution deposition at a temperature of 500 °C for 2 h. For comparison, the films were also ...
Structural, microstructural, optical and electrical properties of (Pb,Ba,Sr)TiO3 films growth on conductive LaNiO3-coated LaAO(3)(100) and Pt/Ti/SiO2/Si substrates
(Elsevier B.V., 2014-04-15)
The ferroelectric and dielectric properties of lead barium strontium titanate (PBST) thin films are investigated on different bottom electrode and substrate such as Pt, LaNiO3 and Pt/Ti/SiO2/Si, LaAlO3(100), respectively. ...
Evaluating mechanisms of adsorbate induced roughening in Si(100) with Monte Carlo simulations
(Springer, 2011-01-27)
Halogen adsorption induces roughening of Si(100) producing pits and regrowth structures that depend on the type of adsorbed halogen and coverage. It is thought that this spontaneous roughening arises from steric repul- ...
Photoluminescence in amorphous (PbLa)TiO3 thin films deposited on different substrates
(2002-08-01)
Pb1-xLaxTiO3 thin films, (X=0.0; 13 and 0.27mol%) were prepared by the polymeric precursor method. Thin films were deposited on Pt/Ti/SiO2/Si(111), Si(100) and glass substrates by spin coating, and annealed in the 200-300°C ...
Photoluminescence in amorphous (PbLa)TiO3 thin films deposited on different substrates
(2002-08-01)
Pb1-xLaxTiO3 thin films, (X=0.0; 13 and 0.27mol%) were prepared by the polymeric precursor method. Thin films were deposited on Pt/Ti/SiO2/Si(111), Si(100) and glass substrates by spin coating, and annealed in the 200-300°C ...
Thickness dependence of structure and piezoelectric properties at nanoscale of polycrystalline lead zirconate titanate thin films
(2013-05-14)
Lead zirconate titanate Pb(Zr0.50Ti0.50)O3 (PZT) thin films were deposited by a polymeric chemical method on Pt(111)/Ti/SiO2/Si substrates to understand the mechanisms of phase transformations and the effect of film thickness ...