dc.contributor | Universidade Estadual Paulista (UNESP) | |
dc.creator | Ries, A. | |
dc.creator | Simoes, A. Z. | |
dc.creator | Cilense, M. | |
dc.creator | Zaghete, M. A. | |
dc.creator | Varela, José Arana | |
dc.date | 2014-05-20T15:27:05Z | |
dc.date | 2016-10-25T18:01:49Z | |
dc.date | 2014-05-20T15:27:05Z | |
dc.date | 2016-10-25T18:01:49Z | |
dc.date | 2003-03-01 | |
dc.date.accessioned | 2017-04-06T00:00:10Z | |
dc.date.available | 2017-04-06T00:00:10Z | |
dc.identifier | Materials Characterization. New York: Elsevier B.V., v. 50, n. 2-3, p. 217-221, 2003. | |
dc.identifier | 1044-5803 | |
dc.identifier | http://hdl.handle.net/11449/37139 | |
dc.identifier | http://acervodigital.unesp.br/handle/11449/37139 | |
dc.identifier | 10.1016/S1044-5803(03)00095-0 | |
dc.identifier | WOS:000186249900021 | |
dc.identifier | http://dx.doi.org/10.1016/S1044-5803(03)00095-0 | |
dc.identifier.uri | http://repositorioslatinoamericanos.uchile.cl/handle/2250/880500 | |
dc.description | Pure barium strontium titanate powder, with Ba/Sr ratio of 80/20 was prepared by the polymeric precursor method (also called Pechini process). The powder was obtained after a calcination at 800 degreesC for 8 h and characterized by XRD, IR, BET and SEM. The requirements to avoid barium carbonate as a secondary phase are presented and discussed in detail. (C) 2003 Elsevier B.V. All rights reserved. | |
dc.language | eng | |
dc.publisher | Elsevier B.V. | |
dc.relation | Materials Characterization | |
dc.rights | info:eu-repo/semantics/closedAccess | |
dc.subject | BST | |
dc.subject | polymeric precursor | |
dc.subject | Pechini | |
dc.subject | microstructure | |
dc.subject | BET | |
dc.title | Barium strontium titanate powder obtained by polymeric precursor method | |
dc.type | Otro | |