dc.creatorZerbino, Jorge Omar
dc.creatorTacconi, Norma R. de
dc.creatorCalandra, Alfredo J.
dc.creatorArvia, Alejandro Jorge
dc.date1977
dc.date2021-05-04T13:46:51Z
dc.date.accessioned2023-07-15T01:35:37Z
dc.date.available2023-07-15T01:35:37Z
dc.identifierhttp://sedici.unlp.edu.ar/handle/10915/118262
dc.identifierissn:1572-6657
dc.identifier.urihttps://repositorioslatinoamericanos.uchile.cl/handle/2250/7458838
dc.descriptionNoble metal electrodes in aqueous solutions under a triangular potential sweep display current peaks due to the electrosorption and electrodesorption of hydrogen and oxygen species [1-7]. In molten bisulphate electrolytes these characteristics were previously observed for platinum [8-11] and are also common for iridium. The electrochemical behaviour of iridium (1 mm diameter wire, Johnson Matthey, 1.0 cm<sup>2</sup> apparent area) was studied in the NaHSO<sub>4</sub>-KHSO<sub>4</sub> melts at 180-300°C using a conventional three compartment electrolysis cell. Its potential was referred to a Pt/H<sub>2</sub>(1 atm)/KHSO<sub>4</sub>(melt) electrode.
dc.descriptionInstituto de Investigaciones Fisicoquímicas Teóricas y Aplicadas
dc.formatapplication/pdf
dc.format379-384
dc.languagees
dc.rightshttp://creativecommons.org/licenses/by-nc-sa/4.0/
dc.rightsCreative Commons Attribution-NonCommercial-ShareAlike 4.0 International (CC BY-NC-SA 4.0)
dc.subjectCiencias Exactas
dc.subjectQuímica
dc.subjectPotentiodynamic behaviour
dc.subjectIridium electrodes
dc.titleThe potentiodynamic behaviour of iridium electrodes in NaHSO<sub>4</sub> - KHSO<sub>4</sub> melts