dc.contributorUniversidade Estadual Paulista (Unesp)
dc.contributorVotorantim Metais/Companhia Brasileira de Aluminio/Rua Moraes do Rego
dc.contributorAMG Brasil/BR 383
dc.date.accessioned2019-10-06T16:13:54Z
dc.date.accessioned2022-12-19T18:45:05Z
dc.date.available2019-10-06T16:13:54Z
dc.date.available2022-12-19T18:45:05Z
dc.date.created2019-10-06T16:13:54Z
dc.date.issued2019-01-01
dc.identifierSolid State Phenomena, v. 285 SSP, p. 224-233.
dc.identifier1662-9779
dc.identifierhttp://hdl.handle.net/11449/188618
dc.identifier10.4028/www.scientific.net/SSP.285.224
dc.identifier2-s2.0-85059941288
dc.identifier.urihttps://repositorioslatinoamericanos.uchile.cl/handle/2250/5369656
dc.description.abstractAl–Si A413 treated and untreated alloys were cast and poured at approximately 720 ºC, 700 ºC, and 680 ºC in a cooling slope to obtain the semisolid material feeding the ceramic nozzle (150 cm 3 ) at the lower roll (single-roll melt-dragged processing)—this drags the metallic slurry via the chill/columnar layers at a rate of 0.2 m/s, forming a molten-metal strip with a thickness of 2 mm and width 45 mm, approximately. The untreated alloy poured at 720 ºC formed coarse structures of α-Al dendrites, as well as a coarse eutectic of Al–Si and microshrinking on the surface of the casting strip facing the atmosphere. The Al–Si 413 alloy poured at 680 ºC and treated with Al5Ti1B (0.1%) led to microstructural refinement, resulting in α-Al globular structures, the absence of microporosities on the surface facing the atmosphere, and a finer and more homogeneous distribution of the eutectic grains with smaller Si particles. The AlTiB master alloys are not used as a grain refiner in Al–Si alloys because of Si poisoning. This subject is discussed in this paper. The addition of the inoculant and 0.2% of the Al–Si eutectic morphology modifying agent (Al–10%Sr) refined both the α-Al and eutectic phases more efficiently in the cast strip poured at 700 ºC and 680 ºC. This suggests that the inoculant did not interfere with the action of the modifying agent. As a result, molten metal strips of higher mechanical strengths and ductilities were obtained.
dc.languageeng
dc.relationSolid State Phenomena
dc.rightsAcesso aberto
dc.sourceScopus
dc.subjectAl-Si A413
dc.subjectAl-Si modification
dc.subjectAl-Sr
dc.subjectAl5Ti1B
dc.subjectCast metallic strips
dc.subjectGrain refining
dc.titleInfluence of pouring temperature and alloy additions on the quality of a semisolid material dragged during the continuous-casting strip processing of al-si a413
dc.typeActas de congresos


Este ítem pertenece a la siguiente institución