Nucleation and growth mechanisms of palladium, nanoflower-shaped, and its performance as electrocatalyst in the reduction of Cr(VI)
dc.creator | Aguirre, María del Carmen | |
dc.date.accessioned | 2021-02-01T19:01:06Z | |
dc.date.accessioned | 2022-10-15T07:38:53Z | |
dc.date.available | 2021-02-01T19:01:06Z | |
dc.date.available | 2022-10-15T07:38:53Z | |
dc.date.created | 2021-02-01T19:01:06Z | |
dc.date.issued | 2019-08-24 | |
dc.identifier | Aguirre, María del Carmen; Nucleation and growth mechanisms of palladium, nanoflower-shaped, and its performance as electrocatalyst in the reduction of Cr(VI); Springer; Journal of Applied Electrochemistry; 49; 8; 24-8-2019; 795-809 | |
dc.identifier | 0021-891X | |
dc.identifier | http://hdl.handle.net/11336/124412 | |
dc.identifier | CONICET Digital | |
dc.identifier | CONICET | |
dc.identifier.uri | https://repositorioslatinoamericanos.uchile.cl/handle/2250/4361347 | |
dc.description.abstract | Palladium electrocrystallization on Ti film is studied through theoretical models of nucleation and growth. At the applied potential + 0.1 V, palladium electrodeposition followed a mechanism through these steps: adsorption, 2D nucleation with ad-atoms incorporation-controlled growth, and 3D nucleation with diffusion-controlled growth. At − 0.3 V, the metallic nucleus and its growth were accompanied by proton reduction, followed by hydrogen adsorption on palladium nucleation sites; thus nucleation turned more progressive. When Pd° was electrodeposited on glassy carbon (GC) electrode at + 0.05 V and + 0.1 V, this led to Volmer–Weber mechanism, with a 3D instantaneous nucleation and diffusion-controlled growth. The structural and morphological characterizations of both substrates determined a Pd° fcc lattice and nanoflowers of Pd° between 100 and 125 nm. Pd/Ti systems are applied in electroanalytic determinations, performing the nanoflowers as highly sensitive electrocatalysts in the chromium(VI) determination in acidic media. Pd/Ti showed a reduction peak at + 0.58 V Ag/AgC in deoxygenated 0.1 mol L−1 H2SO4. Unlike Ti film, the palladium nanostructures contributed to reduction of Cr(VI). Dependence of current peak versus Cr(VI) concentration with Pd/Ti electrocatalysts was linear from 1.9 10−5–10−4 mol L−1, even when the electrode was tested in a real water sample. For comparison, a glassy carbon (GC) electrode and Pd/GC electrode synthesized at + 0.05 V were assayed with Cr(VI). Unlike Ti film, GC contributed to reduction of Cr(VI). Scan rate studies confirmed that Cr(VI) reduction with Pd/Ti is a diffusion-controlled process. Differential pulse voltammetry (DPV) allowed Pd/Ti electrode to obtain a detection limit (LOD) of 5.8 ppb Cr(VI) and a quantitation limit (LOQ) of 19 ppb Cr(VI) in 0.1 mol L−1 H2SO4. | |
dc.language | eng | |
dc.publisher | Springer | |
dc.relation | info:eu-repo/semantics/altIdentifier/url/https://link.springer.com/article/10.1007/s10800-019-01323-0 | |
dc.relation | info:eu-repo/semantics/altIdentifier/doi/https://doi.org/10.1007/s10800-019-01323-0 | |
dc.rights | https://creativecommons.org/licenses/by-nc-sa/2.5/ar/ | |
dc.rights | info:eu-repo/semantics/restrictedAccess | |
dc.subject | CR(VI) DETECTION AND QUANTITATION LIMITS | |
dc.subject | PD NANOFLOWERS | |
dc.subject | PD NUCLEATION AND GROWTH | |
dc.title | Nucleation and growth mechanisms of palladium, nanoflower-shaped, and its performance as electrocatalyst in the reduction of Cr(VI) | |
dc.type | info:eu-repo/semantics/article | |
dc.type | info:ar-repo/semantics/artículo | |
dc.type | info:eu-repo/semantics/publishedVersion |