dc.contributorAfonso, Conrado Ramos Moreira
dc.contributorhttp://lattes.cnpq.br/2176215981291453
dc.contributorhttp://lattes.cnpq.br/0474221317198742
dc.creatorLucena, Felipe Amélio de
dc.date.accessioned2021-06-23T11:51:04Z
dc.date.accessioned2022-10-10T21:35:58Z
dc.date.available2021-06-23T11:51:04Z
dc.date.available2022-10-10T21:35:58Z
dc.date.created2021-06-23T11:51:04Z
dc.date.issued2020-07-28
dc.identifierLUCENA, Felipe Amélio de. Produção de recobrimentos resistentes ao desgaste através de laser cladding de pós das ligas amorfizáveis fe-co-nb-b-(y). 2020. Tese (Doutorado em Ciência e Engenharia de Materiais) – Universidade Federal de São Carlos, São Carlos, 2020. Disponível em: https://repositorio.ufscar.br/handle/ufscar/14412.
dc.identifierhttps://repositorio.ufscar.br/handle/ufscar/14412
dc.identifier.urihttp://repositorioslatinoamericanos.uchile.cl/handle/2250/4044621
dc.description.abstractIndustrial components can be subjected to a high level of surface wear it necessary to search for new wear-resistant alloys to improve the performance and safety of the components. The objective of this work was to produce laser coatings with high hardness and high wear resistance. Three new vitreous alloys of the Fe-Co-Nb-B-Y system were produced in the arc furnace integrated with the suction system using commercial raw materials (Fe-Nb and Fe-B ferroalloys). Subsequently, through the high energy milling process of the splat plates (> 10 cm) generated during gas atomization, powders (∅ <45 μm) were formed for Fe66Co7Nb4B23 and Fe63Co7Nb4B23Y3 (% at.) alloys. Three different coatings (B, C and D) were produced using the Fe66Co7Nb4B23Y3 (% at.) alloy and one coating (A) for the Fe66Co7Nb4B23 (% at.) alloy for comparison. Each coating was produced using different laser parameters and the powders from the milling. The coatings were subjected to the wear test of pin on disk and Vickers hardness. The “A” coating showed a lower average value of the specific wear rate (2.20 x10-5 mm3/Nm) and a higher average value of the friction coefficient (≈ 1.15) compared to “B” coating. The laser remelting process applied over “C” coating and the addition of a second coating layer in the formation of “D” coating did not significantly change its specific wear rates, which were similar in “B” coating (10.9 x 10-5 mm3/Nm). The friction coefficient of “B” coating (≈ 0.5) increased to ≈ 0.7 after its laser remelting for the formation of “C” coating and decreased to ≈ 0.35 in “D” coating with the addition of a second coating layer. The laser cladding process allowed the production of coatings with high hardness (575 ± 60 to 1160 ± 80 HV).
dc.languagepor
dc.publisherUniversidade Federal de São Carlos
dc.publisherUFSCar
dc.publisherPrograma de Pós-Graduação em Ciência e Engenharia de Materiais - PPGCEM
dc.publisherCâmpus São Carlos
dc.rightshttp://creativecommons.org/licenses/by-nc-nd/3.0/br/
dc.rightsAttribution-NonCommercial-NoDerivs 3.0 Brazil
dc.subjectLiga vítrea à base de Fe
dc.subjectPós atomizados
dc.subjectLaser cladding
dc.subjectMicrodureza
dc.subjectDesgaste
dc.subjectFe-based bulk metallic glasses
dc.subjectCoating
dc.subjectWear
dc.subjectPin on disk
dc.subjectMicrohardness
dc.subjectSupercooled liquid
dc.titleProdução de recobrimentos resistentes ao desgaste através de laser cladding de pós das ligas amorfizáveis fe-co-nb-b-(y)
dc.typeTesis