The interest in scientific and technological development of Fe-Mn-Si-Cr-Ni shape memory alloys is increasing in the last years. The improvement of key properties of theses alloys should enable its use in different applications, such as prestressing concrete structures in civil engineering area. In this context, the present work assesses the cerium (Ce) addition to determine its possible benefits in enhancing both corrosion protection in alkaline media and shape memory effect (SME). The studied experimental alloys were subjected to 0.18%, 0.42% and 0.96% (wt%) of Ce addition, and results were compared to a
standard Ce-free alloy. The characterization of such alloys reveals that Ce addition is responsible for a grain size reduction as well as the increase and morphological change in second phase particles. The discussion of the results correlates these microstructural modifications with electrochemical results and
SME. Regarding corrosion properties, all samples presented similar passive behaviors in simulated pore solution in absence of chloride ions. When Cl- was added, the sample with 0.18% was the only one to maintain its passivity while other samples showed a major increase in passive corrosion density, indicating
a worse stability of the passive film. Pit potential and EIS results showed that the addition of 0.18% of Ce was sufficient to enhance corrosion protection by both changing MnS inclusion morphology and increasing the surface film corrosion protection properties, although it was not high enough to promote oxide, sulfides and intermetallic particles that increases localized corrosion appearance. In terms of shape recovery ratio, an increase in samples with 0.18% and 0.42% of Ce was observed, although there was a reduction in
sample with 0.96%. The reduction might be explained by the inhomogeneous microstructure due to the formation of coarse inclusion particles. Finally, the sample with 0.42% presented the best SME results.