Brasil | Artigo
dc.contributorUniversidade Estadual Paulista (Unesp)
dc.contributorUniversity of Zúrich
dc.date.accessioned2014-05-27T11:26:26Z
dc.date.accessioned2022-10-05T18:33:23Z
dc.date.available2014-05-27T11:26:26Z
dc.date.available2022-10-05T18:33:23Z
dc.date.created2014-05-27T11:26:26Z
dc.date.issued2012-04-01
dc.identifierCeramica, v. 58, n. 346, p. 253-261, 2012.
dc.identifier0366-6913
dc.identifier1678-4553
dc.identifierhttp://hdl.handle.net/11449/73247
dc.identifier10.1590/S0366-69132012000200017
dc.identifierS0366-69132012000200017
dc.identifier2-s2.0-84864669954
dc.identifier2-s2.0-84864669954.pdf
dc.identifier.urihttp://repositorioslatinoamericanos.uchile.cl/handle/2250/3922259
dc.description.abstractThis study aimed to evaluate Y-TZP surface after different airborne particle abrasion protocols. Seventy-six Y-TZP ceramic blocks (5×4×4) mm3 were sintered and polished. Specimens were randomly divided into 19 groups (n=4) according to control group and 3 factors: a) protocol duration (2 and 4 s); b) particle size (30 μm, alumina coated silica particle; 45 μm, alumina particle; and 145 μm, alumina particle) and; c) pressure (1.5, 2.5 and 4.5 bar). Airborne particle abrasion was performed following a strict protocol. For qualitative and quantitative results, topography surfaces were analyzed in a digital optical profilometer (Interference Microscopic), using different roughness parameters (Ra, Rq, Rz, X-crossing, Mr1, Mr2 and Sdr) and 3D images. Surface roughness also was analyzed following the primer and silane applications on Y-TZP surfaces. One-way ANOVA revealed that treatments (application period, particle size and pressure of particle blasting) provided significant difference for all roughness parameters. The Tukey test determined that the significant differences between groups were different among roughness parameters. In qualitative analysis, the bonding agent application reduced roughness, filing the valleys in the surface. The protocols performed in this study verified that application period, particle size and pressure influenced the topographic pattern and amplitude of roughness.
dc.languageeng
dc.relationCerâmica
dc.relation0,186
dc.rightsAcesso aberto
dc.sourceScopus
dc.subjectSandblast
dc.subjectSurface modification
dc.subjectZirconia
dc.titleEffect of airborne particle abrasion protocols on surface topography of Y-TZP ceramic