Artigo
Structural characterization of undoped and Sb-doped SnO2 thin films fired at different temperatures
Fecha
2003-06-01Registro en:
Journal of Applied Crystallography. Copenhagen: Blackwell Munksgaard, v. 36, n. 1, p. 736-739, 2003.
0021-8898
10.1107/S0021889803004953
WOS:000182284400076
5584298681870865
9971202585286967
0000-0002-8356-8093
Autor
Universidade Estadual Paulista (Unesp)
Univ Bourgogne
Universidade de São Paulo (USP)
Resumen
SnO2 thin films were obtained by the sol-gel method starting from inorganic precursor solutions. In this work, we compare the structure of undoped and Sb-doped SnO2 films prepared by dip-coating. The films were deposited on quartz substrates and then fired at different temperatures ranging from 383 up to 1173 K. The density and the thickness of the films were determined by X-ray reflectivity (XRR) and their porous nanostructure was characterized by grazing-incidence small angle X-ray scattering (GISAXS). XRR results corresponding to undoped and Sb-doped samples indicate a monotonous decrease in film thickness when they are fired at increasing temperatures. At same time, the apparent density of undoped samples exhibits a progressive increase while for Sb-doped films it remains invariant up to 973 K and then increases for T = 1173 K. Anisotropic GISAXS patterns of both films, Sb-doped and undoped, fired above 573 K indicate the presence of elongated pores with their major axis perpendicular to the film surface. For all firing temperatures the nanopores in doped samples are larger than in undoped ones. This suggests that Sb-doping favours the pore growth hindering the film densification. At the highest firing temperature (1173 K) this effect is reversed.