dc.contributor | Bocchi, Nerilso | |
dc.contributor | http://genos.cnpq.br:12010/dwlattes/owa/prc_imp_cv_int?f_cod=K4783990J3 | |
dc.contributor | http://lattes.cnpq.br/1138611310617865 | |
dc.creator | Silva, Daiane Piva Barbosa da | |
dc.date.accessioned | 2014-12-17 | |
dc.date.accessioned | 2016-06-02T20:34:59Z | |
dc.date.available | 2014-12-17 | |
dc.date.available | 2016-06-02T20:34:59Z | |
dc.date.created | 2014-12-17 | |
dc.date.created | 2016-06-02T20:34:59Z | |
dc.date.issued | 2014-11-28 | |
dc.identifier | SILVA, Daiane Piva Barbosa da. Synthesis and caracterization of lithium and manganese spinels obtained by microwave-assisted hydrothermal route. 2014. 135 f. Tese (Doutorado em Ciências Exatas e da Terra) - Universidade Federal de São Carlos, São Carlos, 2014. | |
dc.identifier | https://repositorio.ufscar.br/handle/ufscar/6328 | |
dc.description.abstract | Lithium and manganese oxide in spinel phase (LiMn2O4) was obtained by microwave-assisted hydrothermal route starting from completely soluble reagents. For this, a mixture of potassium permanganate and lithium hydroxide monohydrate (Li/Mn = 1.2) aqueous solutions and acetone (acetone/Mn = 1.1) was treated in a microwave reactor (850 W) at 140 °C for different times (10 s - 30 min) and under constant magnetic stirring. The obtained materials were characterized by X-ray diffraction, scanning and transmission electron microscopy, X-ray dispersive energy spectroscopy, electrons diffracton, inductively coupled plasma-atomic emission spectroscopy, cyclic voltammetry, thermogravimetry, structural refinement by Rietveld method and chronopotentiometry. The X-ray diffractogramm for the material synthesized in 5 min could be indexed to the JCPDS card number 35-0782 related to the LiMn2O4 in spinel phase, but the unwanted presence of K+ ions in its structure was verified. Thus, an ionic exchange step was included in the process, in which the newly-synthesized material was treated in an aqueous solution of lithium hydroxide in the same microwave reactor for different times (5 - 40 min) and under constant magnetic stirring. After 10 min, a material with low content of K+ ions and Li/Mn ratio = 0.52 was obtained, but it was electrochemically inactive. The material was submitted to a heat treatments in a conventional microwave oven for distinct times (1 - 5 min), having presented, after 4 min, the characteristic electrochemical profile of the spinel. The images obtained by scanning and transmission electron microscopy for this material showed the predominance of prismatic particles with nearly 10 - 25 nm. The results of charge and discharge tests showed that the specific capacity values are strongly dependent of the composite film thickness that composes the electrode. Thinner films presented a value of initial specific capacity of 100 ± 17 mA h g-1 with charge retention of 93% after 75 charge and discharge cycles at C/1 discharge rate. | |
dc.publisher | Universidade Federal de São Carlos | |
dc.publisher | BR | |
dc.publisher | UFSCar | |
dc.publisher | Programa de Pós-Graduação em Química - PPGQ | |
dc.rights | Acesso Aberto | |
dc.subject | Eletroquímica | |
dc.subject | Baterias de lítio | |
dc.subject | Nanomateriais | |
dc.subject | Eletrodos de inserção | |
dc.title | Síntese e caracterização de espinélios de lítio e manganês obtidos via rota hidrotermal assistida por microondas | |
dc.type | Tesis | |