dc.contributor | Universidade Estadual de Campinas (UNICAMP) | |
dc.contributor | Itaúna University | |
dc.contributor | Universidade Estadual Paulista (Unesp) | |
dc.date.accessioned | 2014-05-27T11:23:44Z | |
dc.date.available | 2014-05-27T11:23:44Z | |
dc.date.created | 2014-05-27T11:23:44Z | |
dc.date.issued | 2008-12-01 | |
dc.identifier | Brazilian Dental Journal, v. 19, n. 4, p. 348-353, 2008. | |
dc.identifier | 0103-6440 | |
dc.identifier | 1806-4760 | |
dc.identifier | http://hdl.handle.net/11449/70713 | |
dc.identifier | 10.1590/S0103-64402008000400011 | |
dc.identifier | S0103-64402008000400011 | |
dc.identifier | 2-s2.0-63249129569 | |
dc.identifier | 2-s2.0-63249129569.pdf | |
dc.description.abstract | This study evaluated the effect of microwave energy on the hardness, impact strength and flexural strength of the Clássico, Onda-Cryl and QC-20 acrylic resins. Aluminum die were embedded in metallic or plastic flasks with type III dental stone, in accordance with the traditional packing technique. A mixing powder/liquid ratio was used according to the manufacturer's instructions. After polymerization in water batch at 74°C for 9 h, boiling water for 20 min or microwave energy at 900 W for 10 min, the specimens were deflasked after flask cooling at room temperature, and submitted to finishing. Specimens non-disinfected and disinfected by microwave irradiation were submitted to hardness, impact and flexural strength tests. Each specimen was immersed in distilled water and disinfected in a microwave oven calibrated to 650 W for 3 min. Knoop hardness test was performed with 25 g load for 10 s, impact test was carried out using the Charpy system with 40 kpcm, and 3-point bending test with a crosshead speed of 0.5 mm/min until fracture. Data were submitted to statistical analysis by ANOVA and Tukey's test (α=0.05). Disinfection by microwave energy decreased the hardness of Clássico and Onda-Cryl acrylic resins, but no effect was observed on the impact and flexural strength of all tested resins. | |
dc.language | eng | |
dc.relation | Brazilian Dental Journal | |
dc.relation | 0,476 | |
dc.rights | Acesso aberto | |
dc.source | Scopus | |
dc.subject | Acrylic resin | |
dc.subject | Flexural strength | |
dc.subject | Hardness | |
dc.subject | Impact | |
dc.subject | Microwave disinfection | |
dc.subject | acrylic acid resin | |
dc.subject | dental care | |
dc.subject | disinfection | |
dc.subject | equipment | |
dc.subject | hardness | |
dc.subject | materials testing | |
dc.subject | methodology | |
dc.subject | microwave radiation | |
dc.subject | pliability | |
dc.subject | radiation exposure | |
dc.subject | Acrylic Resins | |
dc.subject | Dental Stress Analysis | |
dc.subject | Disinfection | |
dc.subject | Equipment Contamination | |
dc.subject | Materials Testing | |
dc.subject | Microwaves | |
dc.subject | Pliability | |
dc.title | Effect of microwave disinfection on physical and mechanical properties of acrylic resins | |
dc.type | Artículos de revistas | |