Bonding strength between a hard chairside reline resin and a denture base material as influenced by surface treatment
Fecha
2001-12-01Registro en:
Journal of Oral Rehabilitation. Oxford: Blackwell Publishing Ltd, v. 28, n. 12, p. 1153-1157, 2001.
0305-182X
10.1046/j.1365-2842.2001.00786.x
WOS:000173046100012
8000248781842587
3003130522427820
5737127334248549
8867670539105403
0000-0002-7375-4714
Autor
Universidade Estadual Paulista (Unesp)
Institución
Resumen
Direct relining of dentures made with hard chairside reline resins is faster than laboratory-processed reline systems and the patient is not without the prosthesis for the time necessary to perform the laboratory procedures. However, a weak bond between the autopolymerizing acrylic reline resins and the denture base material has been observed. This study evaluated the effect of six different surface treatments on the bond strength between a hard chairside reline acrylic resin and ia heat-cured acrylic resin. Specimens of the heat-cured acrylic resin were divided into seven groups. one of these groups remained intact. In the other groups, a 10-mm square section was removed from the centre of each specimen. The bonding surfaces were then treated with (i) methyl methacrylate monomer, (ii) isobutyl methacrylate monomer, (iii) chloroform, (iv) acetone, (v) experimental adhesive and (vi) no surface treatment-control group. Kooliner acrylic resin was packed,into the square sections and polymerized. The bonding strength was evaluated by a three-point loading test. The results were submitted to one-way analysis of variance (ANOVA) followed by a Tukey multiple range test at a 5% level of significance. No significant difference was found between the surface treatment with Lucitone 550 monomer or chloroform, but both were stronger than the majority of the other groups. The bond strength provided by all the surface treatments was lower than that of the intact heat-cured resin.