Implementation of an equipment to assess the chemical degradation of MgO-C refractories by the atmosphere at high temperature

dc.creatorMoliné, Marcos Nahuel
dc.date.accessioned2017-08-28T17:37:48Z
dc.date.accessioned2018-11-06T11:38:32Z
dc.date.available2017-08-28T17:37:48Z
dc.date.available2018-11-06T11:38:32Z
dc.date.created2017-08-28T17:37:48Z
dc.date.issued2016-09
dc.identifierMoliné, Marcos Nahuel; Implementación de un equipo para evaluar la degradación química de refractarios MgO-C por la atmósfera a alta temperatura.; Universidad Internacional de la Empresa. Executive Business School; Avances en Ciencias e Ingenieria; 7; 3; 9-2016; 1-10
dc.identifier0718-8706
dc.identifierhttp://hdl.handle.net/11336/23110
dc.identifierCONICET Digital
dc.identifierCONICET
dc.identifier.urihttp://repositorioslatinoamericanos.uchile.cl/handle/2250/1856607
dc.description.abstractSe presenta el diseño y construcción de un equipo para evaluar la corrosión de refractarios sensibles a la atmósfera. Se estudiaron materiales MgO-C, ligados con alquitrán químicamente modificado, con 12 y 8 % p/p de grafito, en atmósferas de argón y aire sintético, a 1000 °C. Los materiales fueron previamente pirolizados a 1000 °C en lecho de grafito, de tal forma que al ser ensayados contenían grafito y carbono residual (proveniente de la resina). Bajo atmósfera inerte (argón) se detectó un muy bajo nivel de reacción. En aire sintético, la mayor pérdida de peso se encontró en el material con mayor contenido de grafito el cual, sin embargo, no llegó a perder la totalidad del carbono durante el ensayo. El porcentaje de carbono oxidado fue proporcionalmente mayor en el refractario con menor contenido de grafito, en el que se perdieron completamente los componentes carbonosos (grafito y carbono residual) antes de finalizar el ensayo.
dc.description.abstractIn particular, this work presents the design and construction of an equipment to evaluate the corrosion of refractories that are sensitive to the surrounding atmosphere. MgO-C materials bonded with chemically modified pitch, with 12 and 8 wt. % of graphite, were studied. Argon and synthetic air were used as testing atmosphere, at a maximum temperature of 1000 °C. The refractories were previously pirolyzed at 1000°C in graphite bed, so that when tested containing residual carbon and graphite (from the resin). Under inert atmosphere (argon), a very low level of reaction was observed. Under synthetic air, the highest weight loss was found in the material with the greater graphite content, which however did not lose all carbon during the test. The percentage of oxidized carbon was proportionally higher in the refractory with the less graphite content, where the carboneous components (graphite and residual carbon) were completely lost before the end of the test.
dc.languagespa
dc.publisherUniversidad Internacional de la Empresa. Executive Business School
dc.relationinfo:eu-repo/semantics/altIdentifier/url/http://www.exeedu.com/publishing.cl/inicio.php?lnk=ctnd&id=366
dc.rightshttps://creativecommons.org/licenses/by-nc-sa/2.5/ar/
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectCORROSIÓN POR GASES
dc.subjectREFRACTARIOS MgO-C
dc.subjectDISEÑO DE EQUIPOS
dc.subjectPÉRDIDAS POR OXIDACIÓN
dc.subjectCORROSION BY GASES
dc.subjectMGO-C REFRACTORIES
dc.subjectEQUIPMENTS DESIGN
dc.subjectOXIDATION LOSSES
dc.titleImplementación de un equipo para evaluar la degradación química de refractarios MgO-C por la atmósfera a alta temperatura.
dc.titleImplementation of an equipment to assess the chemical degradation of MgO-C refractories by the atmosphere at high temperature
dc.typeArtículos de revistas
dc.typeArtículos de revistas
dc.typeArtículos de revistas