Drying behavior and decay resistance of rubberwood from steamed log and presteamed lumber
(2018-07-27)
The objective of this study was to evaluate the effect of log steaming and steaming prior to drying singly and both treatments together on the drying behavior and decay resistance of Hevea brasiliensis wood (rubberwood). ...
Lumber quality of Eucalyptus grandis as a function of diametrical position and log steaming
(Elsevier B.V., 2010-04-01)
The objective of this study was to evaluate the effect of log steaming and of the diametrical position of boards on the timber quality of Eucalyptus grandis. Logs with diameters between 20 and 25 cm, between 25 and 30 cm ...
Lumber quality of Eucalyptus grandis as a function of diametrical position and log steaming
(Elsevier B.V., 2010-04-01)
The objective of this study was to evaluate the effect of log steaming and of the diametrical position of boards on the timber quality of Eucalyptus grandis. Logs with diameters between 20 and 25 cm, between 25 and 30 cm ...
Physical Properties of Wood from Steamed Eucalyptus grandis Logs
(2018-01-01)
This study aimed to evaluate the effect of log steaming on the physical properties of Eucalyptus grandis Hill ex Maiden wood. Logs with diameters between 20 and 25 cm and length of 2.9 m were studied. Half the logs were ...
Chemical properties and decay resistance of eucalyptus grandis wood from steamed logs
(2012-12-01)
The objective of this study was evaluate the effect of the log steaming on the chemical properties and decay resistance of Eucalyptus grandis wood. Logs with diameter between 20 and 22 cm were studied. Half of logs were ...
Chemical properties and decay resistance of eucalyptus grandis wood from steamed logs
(2012-12-01)
The objective of this study was evaluate the effect of the log steaming on the chemical properties and decay resistance of Eucalyptus grandis wood. Logs with diameter between 20 and 22 cm were studied. Half of logs were ...
Temperature charts of Hevea brasiliensis during log steaming and its effect on the board cracks
(Springer, 2014-01-01)
The temperatures of Hevea brasiliensis logs during the steaming process were determined and correlated with the cracks of the boards. Thermocouples were inserted at the center of the logs, and the temperatures were recorded ...
Influência da posição diametral das tábuas e da vaporização nos defeitos de secagem de Eucalyptus grandis
(2007-01-01)
This study evaluated the Eucalyptus grandis drying defects acting on boards diametrical position and on log steaming. Half of the logs, with diameter from 20 to <25, 25 to <30 and 30 to <35cm, were steamed during 20 hours ...
Influência da posição diametral das tábuas e da vaporização nos defeitos de secagem de Eucalyptus grandis
(2007-01-01)
This study evaluated the Eucalyptus grandis drying defects acting on boards diametrical position and on log steaming. Half of the logs, with diameter from 20 to <25, 25 to <30 and 30 to <35cm, were steamed during 20 hours ...