Structural characterization of blends containing both PVDF and natural rubber latex
(Wiley-Blackwell, 2005-12-01)
Films containing different volumes of latex of natural rubber (NR) in a fixed mass of poly (vinylidene fluoride) (PVDF) powder were fabricated by compressing under annealing a mixture of both materials without using any ...
Structural characterization of blends containing both PVDF and natural rubber latex
(Wiley-Blackwell, 2005-12-01)
Films containing different volumes of latex of natural rubber (NR) in a fixed mass of poly (vinylidene fluoride) (PVDF) powder were fabricated by compressing under annealing a mixture of both materials without using any ...
Latex Imaging by Environmental STEM: Application to the Study of the Surfactant Outcome in Hybrid Alkyd/Acrylate System
(American Chemical Society, 2009-06)
Among other uses, latexes are a successful alternative to solvent-borne binders for coatings. Efforts are made to produce hybrid nanostructured latexes containing an acrylic phase and an alkyd phase. However, after film ...
Dispersion of hydroxyapatite nanoparticles in natural rubber latex and poly lactic acid based matrices
(2022-01-01)
Hydroxyapatite (HAp)-polymer composite materials are of interest for materials that interface with or substitute bone tissue. HAp nanoparticles (length 290 nm, width 56 nm) synthesized by a wet chemical method were ...