Osteoconductivity of modified fluorcanasite glass-ceramics for bone tissue augmentation and repair
(WILEY-LISS, 2010)
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na(2)O and CaO or by adding P(2)O(5) to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a ...
In vitro osteogenesis on fluorcanasite glass-ceramic with three different chemical compositions
(SPRINGER, 2008)
This study aimed at investigating in vitro osteogenesis on three fluorcanasite glass-ceramic compositions with different solubilities (K3, K5, and K8). Osteoblastic cells were obtained from human alveolar bone fragments ...
Osteoconductivity of modified fluorcanasite glass-ceramics for bone tissue augmentation and repair
(2010-09-01)
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na 2O and CaO or by adding P 2O 5 to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled ...
Osteoconductivity of modified fluorcanasite glass-ceramics for bone tissue augmentation and repair
(2010-09-01)
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na 2O and CaO or by adding P 2O 5 to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled ...