Microstructural and transport properties of LaNiO3-delta films grown on Si(111) by chemical solution deposition
(Elsevier B.V., 2003-11-24)
Electrically conductive LaNiO3-delta (LNO) thin films with typical thickness of 200 nm were deposited on Si (111) substrates by a chemical solution deposition method and heat-treated in air at 700 degreesC. Structural, ...
Microstructural and transport properties of LaNiO3-delta films grown on Si(111) by chemical solution deposition
(Elsevier B.V., 2003-11-24)
Electrically conductive LaNiO3-delta (LNO) thin films with typical thickness of 200 nm were deposited on Si (111) substrates by a chemical solution deposition method and heat-treated in air at 700 degreesC. Structural, ...
Chemical synthesis and epitaxial growth methods for the preparation of ferroelectric ceramics and thin films
(2018-01-01)
Ferroelectric materials have constantly attracted scientific interest because of their technological applications. The efficiency of ferroelectrics materials is related to the way they are processed because characteristics ...
Chemical deposition of La0.7Ca0.3MnO3±δ films on ceramic substrates
(ABM, ABC, ABPol, 2011-01-01)
In this paper, it is reported the growth of La0.7Ca0.3MnO3±δ films using a chemical solution deposition method (CSD) by the spin-coating technique. Such solution was prepared through a route based on modified polymeric ...
Chemical deposition of La0.7Ca0.3MnO3±δ films on ceramic substrates
(ABM, ABC, ABPol, 2011-01-01)
In this paper, it is reported the growth of La0.7Ca0.3MnO3±δ films using a chemical solution deposition method (CSD) by the spin-coating technique. Such solution was prepared through a route based on modified polymeric ...
Dielectric properties of Ca(Zr0.05Ti0.95)O-3 thin films prepared by chemical solution deposition
(Elsevier B.V., 2006-12-01)
Ca(Zr0.05Ti0.95)O-3 (CZT) thin films were grown on Pt(1 1 1)/Ti/SiO2/Si(1 0 0) substrates by the soft chemical method. The films were deposited from spin-coating technique and annealed at 928 K for 4 h under oxygen atmosphere. ...
Dielectric properties of Ca(Zr0.05Ti0.95)O-3 thin films prepared by chemical solution deposition
(Elsevier B.V., 2006-12-01)
Ca(Zr0.05Ti0.95)O-3 (CZT) thin films were grown on Pt(1 1 1)/Ti/SiO2/Si(1 0 0) substrates by the soft chemical method. The films were deposited from spin-coating technique and annealed at 928 K for 4 h under oxygen atmosphere. ...
Chemical deposition of La0.7Ca0.3MnO3±δ films on ceramic substrates
(ABM, ABC, ABPol, 2014)
Structural and electrical properties of LaNiO3 thin films grown on (100) and (001) oriented SrLaAlO4 substrates by chemical solution deposition method
(2013-09-01)
LaNiO3 thin films were deposited on SrLaAlO4 (1 0 0) and SrLaAlO4 (0 0 1) single crystal substrates by a chemical solution deposition method and heat-treated in oxygen atmosphere at 700° C in tube oven. Structural, ...
Structural and electrical properties of LaNiO3 thin films grown on (100) and (001) oriented SrLaAlO4 substrates by chemical solution deposition method
(2013-09-01)
LaNiO3 thin films were deposited on SrLaAlO4 (1 0 0) and SrLaAlO4 (0 0 1) single crystal substrates by a chemical solution deposition method and heat-treated in oxygen atmosphere at 700° C in tube oven. Structural, ...