Characterization of bismuth titanate ceramics derived by mechanochemical synthesis
(Int Inst Science Sintering (i I S S), 2007-09-01)
Bismuth titanate, Bi(4)Ti(3)O(12) (BIT) nanosized powders have been successfully synthesized via high energy mechanochemical activation. The phase formation of BIT, crystal structure, microstructure, crystallite size and ...
Characterization of bismuth titanate ceramics derived by mechanochemical synthesis
(Int Inst Science Sintering (i I S S), 2007-09-01)
Bismuth titanate, Bi(4)Ti(3)O(12) (BIT) nanosized powders have been successfully synthesized via high energy mechanochemical activation. The phase formation of BIT, crystal structure, microstructure, crystallite size and ...
Ferroelectric and dielectric properties of lanthanum-modified bismuth titanate thin films obtained by the polymeric precursor method
(Kluwer Academic Publ, 2004-07-01)
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), thin films with a La concentration of 0.75 was grown on Pt/Ti/SiO2/Si substrates by using the polymeric precursor solution and spin-coating method. The scanning ...
Synthesis and photocatalytic properties of bismuth titanate with different structures via oxidant peroxo method (OPM)
(Elsevier B.V., 2014-02-01)
Bismuth titanate (Bi4Ti3O12 and Bi12TiO20) Powders were synthesized by the Oxidant Peroxide Method (OPM), and the effect of temperatures on physical and chemical properties of particles was investigated. The results showed ...
Effect of lanthanum and lead doping on the microstructure and visible light photocatalysis of bismuth titanate prepared by the oxidant peroxide method (OPM)
(2015-11-01)
Pure (Bi<inf>12</inf>TiO<inf>20</inf>) and La- and Pb-doped (Bi<inf>12-x</inf>La<inf>x</inf>TiO<inf>20</inf> e Bi<inf>12-x</inf>Pb<inf>x</inf>TiO<inf>20</inf>, with x up to 1.50) bismuth titanates were prepared by the ...
Preparation of lanthanum doped Bi4Ti3O12 ceramics by the polymeric precursor method
(2006-08-01)
Lanthanum-modified bismuth titanate, Bi4 - xLaxTi3O12 (BLT) ceramics, with x ranging from 0 to 0.75 were prepared by the polymeric precursor method. Orthorhombicity of the system is decreased with the increase of lanthanum ...
Preparation of lanthanum doped Bi4Ti3O12 ceramics by the polymeric precursor method
(2006-08-01)
Lanthanum-modified bismuth titanate, Bi4 - xLaxTi3O12 (BLT) ceramics, with x ranging from 0 to 0.75 were prepared by the polymeric precursor method. Orthorhombicity of the system is decreased with the increase of lanthanum ...
Synthesis and characterization of bismuth alkaline titanate powders
(Journal of Alloys and Compounds Volume 509, Issue SUPPL. 1, 14 July 2011, Pages S375-S379, 2011-07-14)
In this work, samples of bismuth alkaline titanate, (K 0.5Na 0.5) (2-x/2)Bi (x/6)TiO 3, (x = 0.05-0.75) have been prepared by conventional ceramic technique and molten salts. Metal oxides or carbonates powders were used ...
Ferroelectric and dielectric properties of lanthanum-modified bismuth titanate thin films obtained by the polymeric precursor method
(Kluwer Academic Publ, 2004-07-01)
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), thin films with a La concentration of 0.75 was grown on Pt/Ti/SiO2/Si substrates by using the polymeric precursor solution and spin-coating method. The scanning ...