Correlative light-electron fractography for fatigue striations characterization in metallic alloys
(2013-09-01)
The correlative light-electron fractography technique combines correlative microscopy concepts to the extended depth-from-focus reconstruction method, associating the reliable topographic information of 3-D maps from light ...
Correlative light-electron fractography for fatigue striations characterization in metallic alloys
(2013-09-01)
The correlative light-electron fractography technique combines correlative microscopy concepts to the extended depth-from-focus reconstruction method, associating the reliable topographic information of 3-D maps from light ...
Three-dimensional analysis of fracture, corrosion and wear surfaces
(PERGAMON-ELSEVIER SCIENCE LTD, 2010)
A brief look at the history of fractography has shown a recent trend in the quantification of topographic parameters through the use of three-dimensional reconstruction techniques, which associate SEM stereoscopy and ...
Quantitative fractography by digital image processing: NIH Image macro tools for stereo pair analysis and 3-D reconstruction
(Blackwell Science, 2001-10-01)
A set of NIH Image macro programs was developed to make qualitative and quantitative analyses from digital stereo pictures produced by scanning electron microscopes. These tools were designed for image alignment, anaglyph ...
Quantitative fractography by digital image processing: NIH Image macro tools for stereo pair analysis and 3-D reconstruction
(Blackwell Science, 2001-10-01)
A set of NIH Image macro programs was developed to make qualitative and quantitative analyses from digital stereo pictures produced by scanning electron microscopes. These tools were designed for image alignment, anaglyph ...
A brief discussion about image quality and SEM methods for quantitative fractography of polymer composites
(2013-05-01)
The methodology for fracture analysis of polymeric composites with scanning electron microscopes (SEM) is still under discussion. Many authors prefer to use sputter coating with a conductive material instead of applying ...
A brief discussion about image quality and SEM methods for quantitative fractography of polymer composites
(2013-05-01)
The methodology for fracture analysis of polymeric composites with scanning electron microscopes (SEM) is still under discussion. Many authors prefer to use sputter coating with a conductive material instead of applying ...
Correlative fractography: Combining scanning electron microscopy and light microscopes for qualitative and quantitative analysis of fracture surfaces
(2013-04-01)
Correlative fractography is a new expression proposed here to describe a new method for the association between scanning electron microscopy (SEM) and light microscopy (LM) for the qualitative and quantitative analysis of ...