The use of fragments of thin veneers as a restorative therapy for anterior teeth disharmony: A case report with 3 years of follow-up
(2012-05-01)
Aim: The present case report described the use of contact lens of thin porcelain veneers as a restorative therapy to solve anterior teeth disharmony. Background: Fragments of thin veneers are minimally invasive restorations ...
The use of fragments of thin veneers as a restorative therapy for anterior teeth disharmony: A case report with 3 years of follow-up
(2012-05-01)
Aim: The present case report described the use of contact lens of thin porcelain veneers as a restorative therapy to solve anterior teeth disharmony. Background: Fragments of thin veneers are minimally invasive restorations ...
Evaluation of procera/porcelain interface in metal-free prosthesis
(2005-12-01)
Prosthetic substructures for dental application are veneered by porcelain comprising a structure with different elastic modulus and thermal expansion coefficients layers. This structure may present residual stresses in ...
Porcelain Veneers as an Alternative for Esthetic Treatment: Clinical Report
(Operative Dentistry IncIndianapolisÍndia, 2013)
Clinical Performance of Porcelain Laminate Veneers: Outcomes of the Aesthetic Pre-evaluative Temporary (APT) Technique
(QUINTESSENCE PUBLISHING CO INCHANOVER PARK, 2012)
This article evaluates the long-term clinical performance of porcelain laminate veneers bonded to teeth prepared with the use of an additive mock-up and aesthetic pre-evaluative temporary (APT) technique over a 12-year ...
Effect of glaze cooling rate on mechanical properties of conventional and pressed porcelain on zirconia
(2016-09-01)
The aim of this study was to characterize a conventional and a pressed porcelain for zirconia core as to biaxial flexural strength (BFS), apparent fracture toughness (FT) and microstructure composition, and to investigate ...
Clinical fractures of veneered zirconia single crowns
(2013-09-01)
Crowns made from an yttria-stabilized tetragonal zirconia polycrystals (3Y-TZP) core with a porcelain veneer have shown high clinical failure rates. Manifestations of clinical failure in veneering ceramic ranges from a ...