Synthesis and physical properties of lipid-based poly(ester-urethane)s, I: Effect of varying polyester segment length
(Elsevier B.V., 2012-08-02)
Four aliphatic thermoplastic poly(ester-urethane)s (PEUs) with similar molecular weights but varying polyesters molecular weight (534-1488 g/mol) were prepared from polyester diols, obtained by melt condensation of Azelaic ...
Synthesis and physical properties of lipid-based poly(ester-urethane)s, I: Effect of varying polyester segment length
(Elsevier B.V., 2012-08-02)
Four aliphatic thermoplastic poly(ester-urethane)s (PEUs) with similar molecular weights but varying polyesters molecular weight (534-1488 g/mol) were prepared from polyester diols, obtained by melt condensation of Azelaic ...
Synthesis and characterization of aliphatic polyesters from glycerol, by-product of biodiesel production, and adipic acid
(2007)
In the present work, polyesters were prepared from the polycondensation between glycerol and adipic acid using dibutyltin dilaurate as catalyst. Three glycerol: adipic acid molar ratio were used for the bulk polymerization ...
Synthesis and characterization of polyesters derived from glycerol and phthalic acid
(2007)
The production of polyester via polycondensation between glycerol and phthalic acid using dibutyltin dilaurate is reported. Three glycerol:phthalic acid molar ratio used for the bulk polymerization were: 2:2; 2:3 and 2:4. ...