Pulsed Nd:YAG laser welding of Ni-alloy Hastelloy C-276 foils
(Elsevier B.V., 2012-01-01)
In this study a pulsed Nd:YAG laser was used to join Hastelloy C-276 thin foil with 100 microns thickness. Pulse energy was varied from 1.0 to 2.25 J at small increments of 0.25 J with a 4 ms pulse duration. The macro and ...
Pulsed Nd:YAG laser welding of Ni-alloy Hastelloy C-276 foils
(Elsevier B.V., 2012-01-01)
In this study a pulsed Nd:YAG laser was used to join Hastelloy C-276 thin foil with 100 microns thickness. Pulse energy was varied from 1.0 to 2.25 J at small increments of 0.25 J with a 4 ms pulse duration. The macro and ...
Pulsed Nd:YAG laser welding of Ni-alloy Hastelloy C-276 foils
(Elsevier B.V., 2014)
Comportamiento microestructural de una superaleación base níquel Hastelloy C-276 expuesta a tratamiento térmico
(Departamento de Metalurgia, 2019)
Se determina el comportamiento microestructural de una superaleación base níquel hastelloy C-276 expuesta a tratamiento térmico. Se realiza
el análisis microscópico del cuerpo de una cuña, preparando muestras con dimensiones ...