Buscar
Mostrando ítems 1-10 de 350
Ceramic repair without hydrofluoric acid
(2016-01-01)
Purpose: To evaluate the bond strength between composite resin and feldspathic ceramic following repair protocols with and without hydrofluoric acid and aging by thermocycling. Materials and Methods: Forty-eight glass ...
Heat treatment of silanized feldspathic ceramic: Effect on the bond strength to resin after thermocycling
(2015-08-10)
Purpose This study aimed to evaluate the effect of heat treatment (at 77 °C) of a silanized feldspathic ceramic on microtensile bond strength (μTBS) with a resin cement before and after being aged by thermocycling. Material ...
Effect of the Etching Duration and Ultrasonic Cleaning on Microtensile Bond Strength Between Feldspathic Ceramic and Resin Cement
(Taylor & Francis Ltd, 2013-03-01)
This study assessed the effect of different etching durations of feldspathic ceramic with hydrofluoric acid (HF) and ultrasonic cleaning of the etched ceramic surface on the microtensile bond strength stability of resin ...
Effect of different impression methods and ceramic materials on adaptation of inlaysEfeito de diferentes métodos de moldagem e materiais cerâmicos na adaptação de inlays
(2018-01-01)
Objective: The aim of this study was to evaluate the internal and marginal adaptation of inlays fabricated from different types of impressions (conventional and digital) and different ceramics (feldspathic and lithium ...
Durability of Microtensile Bond to Nonetched and Etched Feldspar Ceramic: Self-adhesive Resin Cements vs Conventional Resin
(Quintessence Publishing Co Inc, 2011-04-01)
Purpose: The objective of this study was to evaluate the effect of thermocycling (TC), self-adhesive resin cements and surface conditioning on the microtensile bond strength (mu TBS) between feldspathic ceramic blocks and ...
Durability of Microtensile Bond to Nonetched and Etched Feldspar Ceramic: Self-adhesive Resin Cements vs Conventional Resin
(Quintessence Publishing Co Inc, 2011-04-01)
Purpose: The objective of this study was to evaluate the effect of thermocycling (TC), self-adhesive resin cements and surface conditioning on the microtensile bond strength (mu TBS) between feldspathic ceramic blocks and ...
Durability of feldspathic veneering ceramic on glass-infiltrated alumina ceramics after long-term thermocycling.
(2010-07-01)
This study compared the bond strength durability of a feldspathic veneering ceramic to glass-infiltrated reinforced ceramics in dry and aged conditions. Disc shaped (thickness: 4 mm, diameter: 4 mm) of glass-infiltrated ...
Durability of feldspathic veneering ceramic on glass-infiltrated alumina ceramics after long-term thermocycling.
(2010-07-01)
This study compared the bond strength durability of a feldspathic veneering ceramic to glass-infiltrated reinforced ceramics in dry and aged conditions. Disc shaped (thickness: 4 mm, diameter: 4 mm) of glass-infiltrated ...