Buscar
Mostrando ítems 1-10 de 466
The effect of process parameters and cutting tool shape on residual stress of SAE 52100 hard turned steel by high speed machining
(2020-04-26)
This study focused on determining the residual stress of SAE 52100 hard-turned steel. The objective was to evaluate and compare the effects of the cutting-edge geometry and cutting parameters (cutting speed, feed rate, and ...
Residual stress mapping in TiN coatings by nanoindentation technique
(Volume 70, Issue 11, November 2012, Pages 1320-1325, 2012-11)
Abstract
Titanium nitride (TIN) coatings were deposited on American Iron and Steel Institute (AISI) 410 stainless steel substrates by the cathodic arc physical vapor deposition process, varying the substrate bias voltage ...
An evaluation of shot peening, residual stress and stress relaxation on the fatigue life of AISI 4340 steel
(Elsevier B.V., 2002-08-01)
Shot peening is a method widely used to improve the fatigue strength of materials. through the creation of a compressive residual stress field (CRSF) in their surface layers. In the present research the gain in fatigue ...
An evaluation of shot peening, residual stress and stress relaxation on the fatigue life of AISI 4340 steel
(Elsevier B.V., 2002-08-01)
Shot peening is a method widely used to improve the fatigue strength of materials. through the creation of a compressive residual stress field (CRSF) in their surface layers. In the present research the gain in fatigue ...
Residual stresses in TiN, DLC and MoS(2) coated surfaces with regard to their tribological fracture behaviour
(ELSEVIER SCIENCE SA, 2009)
Thin hard coatings on components and tools are used increasingly due to the rapid development in deposition techniques, tribological performance and application skills. The residual stresses in a coated surface are crucial ...
Investigation of residual stress, stress relaxation and work hardening effects induced by shot peening on the fatigue life of AA 6005-T6 aluminum alloy
(2019-01-01)
Fatigue strength improvement of mechanical components is one of the most challenging problems in engineering. One of the known ways to improve fatigue life is by using the shot peening process. However, it is complex to ...
Study on the behavior of the Minimum quantity lubricant - MQL technique under different lubricating and cooling conditions when grinding ABNT 4340 steel
(2005-04-01)
The behavior of the minimum quantity lubricant (MQL) technique was analyzed under different lubricating and cooling conditions when grinding ABNT 4340 steel. The comparative analysis of the residual stress values showed ...
Study on the behavior of the Minimum quantity lubricant - MQL technique under different lubricating and cooling conditions when grinding ABNT 4340 steel
(2005-04-01)
The behavior of the minimum quantity lubricant (MQL) technique was analyzed under different lubricating and cooling conditions when grinding ABNT 4340 steel. The comparative analysis of the residual stress values showed ...