Carbon-coated SnO2 nanobelts and nanoparticles by single catalytic step
(Springer, 2009-05-01)
Several types of carbon nanostructures (amorphous and graphitic), for the coating of SnO2 nanobelts and nanoparticles were obtained by a single catalytic process, during methane, natural gas, and methanol decomposition ...
Carbon-coated SnO2 nanobelts and nanoparticles by single catalytic step
(Springer, 2009-05-01)
Several types of carbon nanostructures (amorphous and graphitic), for the coating of SnO2 nanobelts and nanoparticles were obtained by a single catalytic process, during methane, natural gas, and methanol decomposition ...
Analysis of degradation process during the incorporation of ZrO 2:SiO2 ceramic nanostructures into polyurethane coatings for the corrosion protection of carbon steel
(Journal of Materials Science Volume 48, Issue 3, February 2013, Pages 1067-1084, 2013-02)
Three different molar ratios of ZrO2:SiO2 mixed oxides (25:75, 50:50, 75:25) were produced by the sol-gel technique and sintered at different temperatures (400, 600, 800, and 1000 C) in order to analyze differences in ...
Dispersion of carbon nanotubes in nanostructured epoxy systems forcoating application
(Elsevier Science Sa, 2014-05-28)
This study about the dispersion of carbon nanotubes into an epoxy matrix can be considered as a firstapproach to investigate a potential industrial coating. In order to well disperse carboxylic acid-modifiedmultiwalled ...
Analysis of degradation process during the incorporation of ZrO2:SiO2 ceramic nanostructures intro polyurethane coatings for the corrosion protection of carbon steel
(64th Annual Meeting of the International Society of Electrochemistry- Sep. 2013 Qro. Mex s06-035, 2013-09-13)
Three different molar ratios of ZrO2:SiO2 mixed oxides (25:75, 50:50, 75:25) were produced by the sol-gel technique and sintered at different temperatures (400, 600, 800, and 1000 °C) in order to analyze differenjces in ...
Nanostructured Poly(methyl Methacrylate)-Silica Coatings for Corrosion Protection of Reinforcing Steel
(2022-02-25)
In the absence of preventive maintenance, corrosion of structural steel by the deterioration of the passive layer due to exposure to aggressive environments is the main failure factor of reinforced concrete. To overcome ...
Production of TiO2 Coated Multiwall Carbon Nanotubes by the Sol-Gel Technique
(Univ Fed Sao Carlos, Dept Engenharia Materials, 2017)
In recent years, efforts in developing high strength-low density materials are increasing significantly. One of the promising materials to attend this demand is the carbon nanotube (CNT), to be used mainly as a reinforcing ...