Synthesis of lanthanum silicate apatite-type by sol-gel method using sodium silicate as source of silica

dc.creatorSILVA, F.S.
dc.creatorRODRIGUES, V.G.
dc.creatorMISSO, A.M.
dc.creatorMORAIS, V.R.
dc.creatorYAMAGATA, C.
dc.creatorCONGRESSO BRASILEIRO DE CERAMICA, 60.
dc.date2017-03-24T11:43:08Z
dc.date2017-03-24T11:43:08Z
dc.date15-18 de maio, 2016
dc.date.accessioned2023-09-28T13:33:17Z
dc.date.available2023-09-28T13:33:17Z
dc.identifierhttp://repositorio.ipen.br/handle/123456789/27312
dc.identifier.urihttps://repositorioslatinoamericanos.uchile.cl/handle/2250/8997589
dc.descriptionCeramics of lanthanum silicate apatite-type have been studied with great technological interest at IT-SOFC applications (Intermediate Temperature Solid Oxide Fuel Cell) for having good ionic conductivity at intermediate temperatures (600-800??C), higher than that of YSZ (Ytria Stabilized Zirconia) in high-temperature SOFCs. At this work has made the synthesis of the lanthanum silicate apatite-type from Na2SiO3 as a source of silica by the modified sol-gel method that allowed the formation of ceramic powders of lanthanum silicate apatite-type in calcination temperature at 900??C, which is much lower than those other methods of synthesis. Analysis by x-ray diffraction (XRD) showed the lanthanum silicate apatite-type phase as the main phase. Scanning electron microscopy was used to nanometric powders observation.
dc.format156-167
dc.rightsopenAccess
dc.titleS??ntese de silicato de lant??nio tipo apatita pelo m??todo sol-gel utilizando silicato de s??dio como fonte de s??lica
dc.titleSynthesis of lanthanum silicate apatite-type by sol-gel method using sodium silicate as source of silica