| dc.contributor | Universidade Estadual Paulista (UNESP) | |
| dc.creator | Fernandes, Aline Úrsula Rocha | |
| dc.creator | Goiato, Marcelo Coelho | |
| dc.creator | Santos, Daniela Micheline dos | |
| dc.date | 2014-05-27T11:24:41Z | |
| dc.date | 2016-10-25T18:28:40Z | |
| dc.date | 2014-05-27T11:24:41Z | |
| dc.date | 2016-10-25T18:28:40Z | |
| dc.date | 2010-06-01 | |
| dc.date.accessioned | 2017-04-06T01:41:24Z | |
| dc.date.available | 2017-04-06T01:41:24Z | |
| dc.identifier | Contact Lens and Anterior Eye, v. 33, n. 3, p. 124-127, 2010. | |
| dc.identifier | 1367-0484 | |
| dc.identifier | 1476-5411 | |
| dc.identifier | http://hdl.handle.net/11449/71696 | |
| dc.identifier | http://acervodigital.unesp.br/handle/11449/71696 | |
| dc.identifier | 10.1016/j.clae.2009.12.008 | |
| dc.identifier | 2-s2.0-77952891112 | |
| dc.identifier | 0000-0002-3800-3050 | |
| dc.identifier | http://dx.doi.org/10.1016/j.clae.2009.12.008 | |
| dc.identifier.uri | http://repositorioslatinoamericanos.uchile.cl/handle/2250/892644 | |
| dc.description | Purpose: The aim of this study was to evaluate the roughness of colorless ocular button and four brands of colorless acrylic resins designed to fabricate ocular prosthesis as a function of weathering (1008 h) and different thickness (1 and 3.5 mm). Materials and methods: One-hundred-and-twenty specimens were fabricated and distributed in 12 groups. The analysis was carried out by means of digital roughness meter. Results: Data were analyzed statistically by ANOVA and Tukey test at 1% significance. The results showed that there was no statistically significant difference after the weathering period. Both the Vipi Cril acrylic resin with 3.5 mm in thickness and ocular button with 1 mm in thickness presented the lowest roughness values (0.12. Ra). Conclusion: The roughness of the acrylic resins and the ocular button was not affect by the weathering of 1008 h. However, the thickness of the specimens proved to have a major influence on roughness property. © 2010. | |
| dc.language | eng | |
| dc.relation | Contact Lens and Anterior Eye | |
| dc.rights | info:eu-repo/semantics/closedAccess | |
| dc.subject | Ocular prosthesis | |
| dc.subject | Roughness | |
| dc.subject | Thickness | |
| dc.subject | Weathering | |
| dc.subject | acrylic acid resin | |
| dc.subject | ethylene glycol dimethacrylate | |
| dc.subject | methacrylic acid | |
| dc.subject | methacrylic acid methyl ester | |
| dc.subject | controlled study | |
| dc.subject | materials testing | |
| dc.subject | polymerization | |
| dc.subject | priority journal | |
| dc.subject | prosthesis material | |
| dc.subject | surface property | |
| dc.subject | thickness | |
| dc.subject | visual prosthesis | |
| dc.subject | Acrylic Resins | |
| dc.subject | Biocompatible Materials | |
| dc.subject | Contact Lenses | |
| dc.subject | Equipment Design | |
| dc.subject | Equipment Failure Analysis | |
| dc.subject | Hardness | |
| dc.subject | Materials Testing | |
| dc.subject | Surface Properties | |
| dc.title | Effect of weathering and thickness on roughness of acrylic resin and ocular button | |
| dc.type | Otro | |