dc.contributor | Universidade Estadual Paulista (UNESP) | |
dc.creator | Vernilli Jr., Fernando | |
dc.creator | Justus, Sérgio Murilo | |
dc.creator | Silva, Sidiney Nascimento | |
dc.creator | Mazine, Alex | |
dc.creator | Baldo, João Batista | |
dc.creator | Longo, Elson | |
dc.creator | Varela, José Arana | |
dc.date | 2014-05-27T11:21:14Z | |
dc.date | 2016-10-25T18:20:18Z | |
dc.date | 2014-05-27T11:21:14Z | |
dc.date | 2016-10-25T18:20:18Z | |
dc.date | 2004-12-01 | |
dc.date.accessioned | 2017-04-06T01:11:48Z | |
dc.date.available | 2017-04-06T01:11:48Z | |
dc.identifier | 2nd International Meeting on Ironmaking and 1st International Symposium on Iron Ore and Parallel Event- 5th Japan-Brazil Symposium on Dust Processing-Energy-Environment on Metallurgical Industries, v. 1, p. 133-144. | |
dc.identifier | http://hdl.handle.net/11449/68060 | |
dc.identifier | http://acervodigital.unesp.br/handle/11449/68060 | |
dc.identifier | 2-s2.0-33644974572 | |
dc.identifier.uri | http://repositorioslatinoamericanos.uchile.cl/handle/2250/889442 | |
dc.description | This paper investigates corrosion behavior in graphite refractory hot metal impregnated with ZrO 2 and CeO 2 carrying solutions used in Blast Furnace hearth, consisting of 50% graphite and 50% anthracite. Corrosions tests were carried out by means of finger test method in an induction furnace, using bar-shaped 30×30×280 mm test specimens and hot metal from CSN#2 Blast Furnace runner. The temperature chosen for this test was 1520°C and sixty-minute isotherm. Upon test completion, test specimens were characterized by their dimensional variation, X-ray diffractometry and Scanning Electronic Microscopy (SEM). | |
dc.language | eng | |
dc.relation | 2nd International Meeting on Ironmaking and 1st International Symposium on Iron Ore and Parallel Event- 5th Japan-Brazil Symposium on Dust Processing-Energy-Environment on Metallurgical Industries | |
dc.rights | info:eu-repo/semantics/closedAccess | |
dc.subject | Ceria | |
dc.subject | Corrosion | |
dc.subject | Graphite | |
dc.subject | Hot metal | |
dc.subject | Zirconia | |
dc.subject | Sixty-minute isotherm | |
dc.subject | Cerium compounds | |
dc.subject | Impregnation | |
dc.subject | Isotherms | |
dc.subject | X ray diffraction | |
dc.subject | Refractory materials | |
dc.title | Corrosion behavior in graphite refractories impregnated with ZrO 2 and CeO 2 carrying solutions | |
dc.type | Otro | |