Calorimetric and SEM studies of PHB-PET polymeric blends
Registro en:
Journal of Thermal Analysis and Calorimetry. Dordrecht: Springer, v. 97, n. 2, p. 581-584, 2009.
1388-6150
10.1007/s10973-009-0328-5
WOS:000271108200035
0000-0002-7984-5908
Autor
Dias, D. S.
Crespi, Marisa Spirandeli
Kobelnik, M.
Ribeiro, Clovis Augusto
Resumen
PHB [poly (3-hydroxybutyrate)], post-consumer soft-drink bottles poly (ethylene terephthalate) PET (herein named PET-R) and PHBPET-R (blends of PHB and PET-R in several compositions) samples were evaluated by differential scanning calorimetry (DSC) and scanning electronic microscopy (SEM) in order to verify their thermal properties and porosity according to amounts of PET-R added the blends. The DSC curve showed that the solvents used to solve the polymer mixture cause changes in the thermal behavior of PET-R films and in PHBPET-R blends. SEM studies of the PHBPET-R blends show that with a gradual mass increase of PET-R, there are gradual increases in the porosity of the films. Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)