dc.contributorUniversidade Estadual Paulista (UNESP)
dc.creatorLopes, A. G.
dc.creatorNeisser, M. P.
dc.creatorLeite, F.
dc.creatorOlivieri, K. A. N.
dc.creatorAvelar, R. P.
dc.creatorDias, A. H.
dc.date2014-05-20T15:27:09Z
dc.date2016-10-25T18:01:55Z
dc.date2014-05-20T15:27:09Z
dc.date2016-10-25T18:01:55Z
dc.date2003-06-01
dc.date.accessioned2017-04-06T00:00:37Z
dc.date.available2017-04-06T00:00:37Z
dc.identifierJournal of Dental Research. Alexandria: Int Amer Associação Dental Researchi A D R/a A D R, v. 82, p. B337-B337, 2003.
dc.identifier0022-0345
dc.identifierhttp://hdl.handle.net/11449/37195
dc.identifierhttp://acervodigital.unesp.br/handle/11449/37195
dc.identifierWOS:000202893603277
dc.identifierhttp://jdr.sagepub.com/content/82/1_suppl/B13
dc.identifier.urihttp://repositorioslatinoamericanos.uchile.cl/handle/2250/880554
dc.languageeng
dc.publisherInt Amer Assoc Dental Researchi
dc.relationJournal of Dental Research
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.titleMicrotensile bond strength between a glass-infiltrated alumina ceramic, with and without the application of a silane coupling agent, and a resin cement.