dc.contributorUniversidade Estadual Paulista (UNESP)
dc.creatorVercik, L. C. de O.
dc.creatorAssis, C. M. de
dc.creatorFook, M. V. Lia
dc.creatorSantos, M. L. dos
dc.creatorGuastaldi, Antonio Carlos
dc.date2014-05-20T14:18:50Z
dc.date2016-10-25T17:40:46Z
dc.date2014-05-20T14:18:50Z
dc.date2016-10-25T17:40:46Z
dc.date2003-01-01
dc.date.accessioned2017-04-05T22:29:33Z
dc.date.available2017-04-05T22:29:33Z
dc.identifierEclética Química. Fundação Editora da Universidade Estadual Paulista Júlio de Mesquita Filho - UNESP, v. 28, n. 1, p. 25-31, 2003.
dc.identifier0100-4670
dc.identifierhttp://hdl.handle.net/11449/25679
dc.identifierhttp://acervodigital.unesp.br/handle/11449/25679
dc.identifier10.1590/S0100-46702003000100003
dc.identifierS0100-46702003000100003
dc.identifierS0100-46702003000100003.pdf
dc.identifierhttp://dx.doi.org/10.1590/S0100-46702003000100003
dc.identifier.urihttp://repositorioslatinoamericanos.uchile.cl/handle/2250/870538
dc.descriptionTitânio comercialmente puro, Ti-cp, e algumas de suas ligas são consideradas muito importantes na área médica devido sua excelente biocompatibilidade e propriedades mecânicas. Recentemente, foi desenvolvido um método químico, relativamente simples, para induzir a bioatividade desses materiais metálicos inertes, cujo princípio é imitar as condições biológica para obtenção do material desejado. Esta técnica denominada biomimético, foi utilizada para modificar a superfície do Ti-cp através do depósito de uma camada de apatita. O objetivo principal deste trabalho foi estudar a influência do tratamento térmico na evolução da cristalinidade das fases depositadas. Os recobrimentos de apatitas, com tratamentos térmicos entre 400 e 600 ºC, mostraram através das técnicas de difração de raios-X e microscopia eletrônica de varredura, uma baixa cristalinidade semelhante às apatitas biológicas. Acima de 700 ºC, os recobrimentos de apatita mostraram-se mais cristalinos apresentando uma mistura de fases de hidroxiapatita, fosfato octacálcico e fosfato de magnésio.
dc.descriptionCommercially pure titanium (cp-Ti), and some of its alloys are considered very important in the medical field because of its excellent biocompatibility and mechanical properties. Recently a simple chemical method was introduced to induce the bioactivity of these inert metallic materials. In this work, the biomimetic chemical process has been used to modify the cp-Ti surface with the deposit of a layer of apatite. The main objective consisted in studying the influence of the thermal treatment on the evolution of the crystallinity of the deposited phases. X-ray diffraction and scanning electron microscopy techniques showed that the apatite coatings with thermal treatments between 400 and 600 ºC presented low crystallinity similar to the biological apatites. Above 700 ºC, the apatite coatings appeared more crystalline, exhibiting a mixture of hydroxyapatite, octacalcium phosphate and magnesium phosphate.
dc.descriptionFundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
dc.descriptionConselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
dc.descriptionCoordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
dc.languagepor
dc.publisherEditora Unesp
dc.relationEclética Química
dc.rightsinfo:eu-repo/semantics/openAccess
dc.subjectBiomateriais
dc.subjecttitânio
dc.subjectrecobrimento
dc.subjectprocesso biomimético
dc.subjecthidroxiapatita
dc.subjectBiomaterials
dc.subjecttitanium
dc.subjectcoatings
dc.subjectbiomimetic process
dc.subjecthydroxyapatite
dc.titleRecobrimento de apatitas in vitro sobre titânio: influência do tratamento térmico
dc.typeOtro


Este ítem pertenece a la siguiente institución