dc.contributorUniversidade Estadual Paulista (UNESP)
dc.creatorMalta, D. A. M. P.
dc.creatorCosta, M. M.
dc.creatorPelino, J. E. P.
dc.creatorde Andrade, M. E.
dc.creatorLizarelli, R. F. Z.
dc.date2014-05-20T13:47:11Z
dc.date2016-10-25T17:00:41Z
dc.date2014-05-20T13:47:11Z
dc.date2016-10-25T17:00:41Z
dc.date2008-02-01
dc.date.accessioned2017-04-05T20:56:49Z
dc.date.available2017-04-05T20:56:49Z
dc.identifierLaser Physics Letters. Weinheim: Wiley-v C H Verlag Gmbh, v. 5, n. 2, p. 144-150, 2008.
dc.identifier1612-2011
dc.identifierhttp://hdl.handle.net/11449/16758
dc.identifierhttp://acervodigital.unesp.br/handle/11449/16758
dc.identifier10.1002/lapl.200710089
dc.identifierWOS:000253255400011
dc.identifierhttp://dx.doi.org/10.1002/lapl.200710089
dc.identifier.urihttp://repositorioslatinoamericanos.uchile.cl/handle/2250/863471
dc.descriptionThe purpose of this in vitro study was to verify through micro tensile bond test the bond strength of an adhesive system irradiated with Nd:YAG laser in dentine previously treated with Er:YAG laser. Twenty caries free extracted human third molars were used. The teeth were divided in four experimental groups (n = 5): (G1) control group; (G2) irradiation of the adhesive system with the Nd:YAG laser; (G3) dentin treatment with Er:YAG laser; (G4) dentin treatment with Er:YAG laser followed by the irradiation of the adhesive system with Nd:YAG laser. The Er:YAG laser fluency parameter for the dentin treatment was of 60 J/cm(2). ne adhesive system was irradiated with the Nd:YAG laser with fluency of 100 J/cm(2). Dental restorations were performed with Adper Single Bond 2/Z250. One tooth from each group was prepared for the evaluation of the adhesive interface under SEM and bond failure tests were also performed and evaluated. The statistical analysis showed statistical significant difference between the groups G1 and G3, G1 and G4, G2 and G3, and G2 and G4; and similarity between the groups G1 and G2, and G3 and G4. The adhesive failures were predominant in all the experimental groups. The SEM analysis showed an adhesive interface with features confirming the results of the mechanical tests. The Nd:YAG laser on the adhesive system did not influence the bond strength in dentin treated or not with the Er:YAG laser.
dc.languageeng
dc.publisherWiley-v C H Verlag Gmbh
dc.relationLaser Physics Letters
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectadhesion
dc.subjectdentin
dc.subjectEr : YAG laser
dc.subjectNd : YAG laser
dc.subjectmicrotensile bond strength
dc.titleBond strength of an adhesive system irradiated with Nd : YAG laser in dentin treated with Er : YAG laser