dc.creator | MAY LOZANO, MARCOS; 63284 | |
dc.creator | CHIÑAS LOPEZ, SERGIO GEOVANNI; 897835 | |
dc.creator | LOPEZ MEDINA, RICARDO; 44531 | |
dc.creator | Rojas Garcia, Elizabeth;#0000-0003-3973-352X | |
dc.creator | Martínez Delgadillo, Sergio Alejandro; 10682 | |
dc.creator | GONZALEZ REYES, LEONARDO; 160168 | |
dc.creator | May Lozano, Marcos | |
dc.creator | Chiñas López, Sergio Geovanni. | |
dc.creator | López Medina, Ricardo | |
dc.creator | Rojas García, Elizabeth | |
dc.creator | Martínez Delgadillo, Sergio Alejandro | |
dc.creator | González Reyes, Leonardo | |
dc.date.accessioned | 2022-06-03T19:41:13Z | |
dc.date.accessioned | 2022-10-14T13:51:31Z | |
dc.date.available | 2022-06-03T19:41:13Z | |
dc.date.available | 2022-10-14T13:51:31Z | |
dc.date.created | 2022-06-03T19:41:13Z | |
dc.date.issued | 2015 | |
dc.identifier | http://hdl.handle.net/11191/8866 | |
dc.identifier.uri | https://repositorioslatinoamericanos.uchile.cl/handle/2250/4239845 | |
dc.description.abstract | Fe₂O₃-TiO₂ (1% de Fe) y muestras de TiO₂ puro (como referencia) fueron sintetizados por el método sol-gel. Los catalizadores Fe₂O₃-TiO₂ se prepararon para obtener un contenido de 1% de hierro. El TiO₂ sintetizado fue mezclado y molido con nanopartículas Fe₂O₃. Se determinó su estructura cristalográfica, parámetros de red y tamaño de partícula por difracción de rayos X. El área específica y diámetro de poro fueron determinados por el método BET (N₂ adsorción). Además, se realizaron estudios de degradación mediante reacciones fotocatalíticas y sono-fotocatalíticas, en la degradación del colorante Orange II (ultrasonido 250, 500 y 1000 kHz). Los materiales calcinados mostraron ser nanopartículas mesoporosas de TiO₂ en fase anatasa, con excelentes propiedades sonofotocatalíticas. La mejor actividad sono-fotocatalítica resultante fue mediante el uso de ultrasonido de 500 KHz. La longitud de onda de la fuente de luz no fue importante en las reacciones fotocatalíticas. | |
dc.description.abstract | Fe₂O₃-TiO₂ (1% Fe) samples and pure TiO₂ (as reference) were synthesized by the sol gel method. The Fe₂O₃-TiO₂ catalysts were prepared to obtain a content of 1% of iron. The synthesized TiO₂ was mixed and ground with Fe₂O₃ nanoparticles. Their crystallographic structure, lattice parameters and particle size were determined by X-ray diffraction. The specific area and pore diameter was studied by BET method (N2 adsorption). In addition, degradation studies using Orange II dye sono-photocatalysis were performed (ultrasound 250, 500 and 1000 kHz). The calcined materials showed TiO₂ nanoparticles in anatase phase and the mesoporous structures showed excellent sono-photocatalytic properties. Best sono-photocatalytic activity resulted with the use of ultrasound to 500 KHz. The wavelength of the light source was not important in photocatalytic reactions. | |
dc.language | spa | |
dc.publisher | Universidad Autónoma Metropolitana (México). Unidad Azcapotzalco. División de Ciencias Básicas e Ingeniería. | |
dc.rights | http://creativecommons.org/licenses/by-nc-nd/4.0 | |
dc.rights | openAccess | |
dc.rights | Atribución-NoComercial-SinDerivadas | |
dc.source | Revista Tendencias en Docencia e Investigación en Química. Año 1, número 1 (enero-diciembre de 2015). ISSN: 2448-6663 | |
dc.subject | Fe₂O₃-TiO₂, ultrasonido, sono-fotocatálisis. | |
dc.title | Degradación sono-fotocatalítica de orange II usando Fe₂O₃-TiO₂ | |
dc.type | Artículo | |