dc.descriptionIn this paper, we report the electrochemical polymerization of 3-decylthiophene at room temperature using the l-butyl-3-methylimidazoliumtetrafluorborate as solvent. The polymer film is electroactive and its morphology depends upon the anode used. The polymerized 3-decylthiophene was characterized by ft-infrared, uv-visible, thermal gravimetric analysis and conductivity measurement
dc.formattext/html
dc.languageen
dc.publisherSociedad Chilena de Química
dc.sourceJournal of the Chilean Chemical Society v.52 n.3 2007
dc.subjectpolythiophene
dc.subjectelectropolymerization
dc.subjectionic solvent
dc.subjectconducting polymer
dc.titleMORPHOLOGICAL AND STRUCTURAL CHARACTERIZATION OF POLY(3-DECYLTHIOPHENE) PREPARED BY ELECTROPOLYMERIZATION USING 1-BUTYL-3-METHYL-IMIDAZOLIUMTETRAFLUORBORATE AS SOLVENT