Artigo
Fatigue resistance of the bond of a glass-infiltrated alumina ceramic to human dentin
Fecha
2006-05-09Registro en:
Journal of Adhesive Dentistry, v. 8, n. 2, p. 97-104, 2006.
1461-5185
10.3290/j.jad.a11071
WOS:000236862200005
2-s2.0-33646260212
9234456003563666
Autor
University of Bologna
Federal University of Santa Maria
University of Siena
Universidade Estadual Paulista (Unesp)
Dept. of Restorative Dentistry
Resumen
Purpose: To evaluate the fatigue resistance of the bond between dentin and glass-infiltrated alumina ceramic, using different luting protocols. Materials and Methods: The null hypothesis is that the fatigue resistance varies with the luting strategy. Forty blocks of In-Ceram Alumina were prepared, and one surface of each block was abraded with 110-μm aluminum oxide particles. Then, the blocks were luted to flat dentin surfaces of 40 human third molars, using 4 different luting strategies (luting system [LS]/ceramic surface conditioning [CSC]) (n=10): (G1) [LS] RelyX-Unicem/[CSC] airborne abrasion with 110-μm Al2O3 particles; (G2) [LS] One-Step + Duo-Link (bis-GMA-based resin)/[CSC] etching with 4% hydrofluoric acid + silane agent; (G3) [LS] ED-Primer + Panavia F (MDP-based resin)/[CSC] Al2O 3; (G4) [LS] Scotchbond1+RelyX-ARC (bis-GMA-based resin)/[CSC] chairside tribochemical silica coating (air abrasion with 30-μm SiO x particles + silane). After 24 h of water storage at 37°C, the specimens were subjected to 106 fatigue cycles in shear with a sinusoidal load (0 to 21 N, 8 Hz frequency, 37°C water). A fatigue survivor score was given, considering the number of the fatigue cycles until fracture. The failure modes of failed specimens were observed in a SEM. Results: G3 (score = 5.9, 1 failure) and G4 (score = 6, no failures) were statistically similar (p = 0.33) and had significantly higher fatigue resistance than G1 (score = 3.9, 5 failures) and G2 (score = 3.7, 6 failures) (p < 0.03). SEM analysis of fractured specimens of G1 and G2 showed that almost all the failures were between ceramic and cement. Conclusion: The MDP-based resin cement + sandblasting with Al2O3 particles (G3) and bis-GMA-based resin cement + tribochemical silica coating (G4), both using the respective dentin bonding systems, were the best luting protocols for the alumina ceramic. The null hypothesis was confirmed.
Materias
Ítems relacionados
Mostrando ítems relacionados por Título, autor o materia.
-
Fatigue resistance of the bond of a glass-infiltrated alumina ceramic to human dentin
Baldissara, Paolo; Valandro, Luiz Felipe; Monaco, Carlo; Ferrari, Marco; Bottino, Marco Antonio; Scotti, Roberto -
Fatigue resistance of the bond of a glass-infiltrated alumina ceramic to human dentin
University of Bologna; Federal University of Santa Maria; University of Siena; Universidade Estadual Paulista (Unesp); Dept. of Restorative Dentistry (2006-05-09)Purpose: To evaluate the fatigue resistance of the bond between dentin and glass-infiltrated alumina ceramic, using different luting protocols. Materials and Methods: The null hypothesis is that the fatigue resistance ... -
Effects of cement-curing mode and light-curing unit on the bond durability of ceramic cemented to dentin
Passos, Sheila Pestana; Souza, Rodrigo Othávio Assunção; Michida, Silvia Masae Araújo; Zamboni, Sandra Costa; de Oliveira, Simone Helena Gonçalves