Influence of activation modes on diametral tensile strength of dual-curing resin cements.
Fecha
2005-10-01Registro en:
Brazilian oral research, v. 19, n. 4, p. 267-271, 2005.
1806-8324
10.1590/S1806-83242005000400006
S1806-83242005000400006
2-s2.0-36048947965
2-s2.0-36048947965.pdf
3041561340615890
2851339311179809
Autor
Universidade Estadual Paulista (Unesp)
Resumen
In metallic restorations, the polymerization of dual-curing resin cements depends exclusively on chemical activation. The effect of the lack of photoactivation on the strength of these cements has been rarely studied. This study evaluated the influence of activation modes on the diametral tensile strength (DTS) of dual-curing resin cements. Base and catalyst pastes of Panavia F, Variolink II, Scotchbond Resin Cement, Rely X and Enforce were mixed and inserted into cylindrical metal moulds (4 x 2 mm). Cements were either: 1) not exposed to light (chemical activation = self-cured groups) or 2) photoactivated through mylar strips (chemical and photo-activation = dual-cured groups) (n = 10). After a 24 h storage in 37 masculineC distilled water, specimens were subjected to compressive load in a testing machine. A self-curing resin cement (Cement-It) and a zinc phosphate cement served as controls. Comparative analyses were performed: 1) between the activation modes for each dual-curing resin cement, using Students t test; 2) among the self-cured groups of the dual-curing resin cements and the control groups, using one-way ANOVA and Tukeys test (alpha = 0.05). The dual-cured groups of Scotchbond Resin Cement (53.3 MPa), Variolink II (48.4 MPa) and Rely X (51.6 MPa) showed higher DTS than that of self-cured groups (44.6, 40.4 and 44.5 MPa respectively) (p < 0.05). For Enforce (48.5 and 47.8 MPa) and Panavia F (44.0 and 43.3 MPa), no significant difference was found between the activation modes (p > 0.05). The self-cured groups of all the dual-curing resin cements presented statistically the same DTS as that of Cement-It (44.1 MPa) (p > 0.05), and higher DTS than that of zinc phosphate (4.2 MPa). Scotchbond Resin Cement, Variolink II and Rely X depended on photoactivation to achieve maximum DTS. In the absence of light, all the dual-curing resin cements presented higher DTS than that of zinc phosphate and statistically the same as that of Cement-It (p > 0.05).
Materias
Ítems relacionados
Mostrando ítems relacionados por Título, autor o materia.
-
Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading
Özcan, Mutlu; Melo, Renata M.; Souza, Rodrigo O.A.; Machado, João P.B.; Felipe Valandro, Luiz; Botttino, Marco A. -
Muscular Strength as a Predictor of All-Cause Mortality in an Apparently Healthy Population: A Systematic Review and Meta-Analysis of Data From Approximately 2 Million Men and Women
García-Hermoso A.; Cavero-Redondo I.; Ramírez-Vélez R.; Ruiz J.R.; Ortega F.B.; Lee D.-C.; Martínez-Vizcaíno V. (W.B. Saunders, 2018) -
Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading
Clinic for Fixed and Removable Prosthodontics and Dental Materials Science; Universidade Estadual Paulista (Unesp); Division of Prosthodontics; National Institute of Spatial Research (2013-04-01)This study evaluated the effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading. Disc-shaped zirconia specimens (Ø: ...