Resumen
BaTiO(3) powders were prepared through mechanical activation chemistry and analyzed by Rietveld refinement with X-ray diffraction data. Raw BaCO(3) and TiO(2) powders were dry milled for 5 and 20 h and then calcinated for 2 and 4 h at 800 degrees C. The milling process was found to have broken up the BaCO(3) and TiO(2) crystals into smaller crystals and formed only small amounts ( 1.5 wt%) of BaTiO(3). Subsequence calcinations for 2 and 4 h at 800 degrees C successfully produced large amounts (>97.7 wt%) of BaTiO(3) crystals. The calcination process also generated microstrains and crystallite-size anisotropy in BaTiO(3). An increase in the calcination time from 2 to 4 h increased the BaTiO(3) weight percentage and the crystal lite-shape anisotropy, but decreased the tetragonal distortion anisotropic microstrains in BaTiO(3) crystals. (C) 2008 International Centre for Diffraction Data.