Effects of Self-Etching Adhesive Systems Used in the Dental Modelling Technique on the Cohesive Strength of Composite Resin
Fecha
2011-01-01Registro en:
Journal of Adhesion. Abingdon: Taylor & Francis Ltd, v. 87, n. 2, p. 154-161, 2011.
0021-8464
10.1080/00218464.2011.545340
WOS:000287299200004
3135367849609938
1754020652874850
0000-0003-4830-0400
Autor
Universidade Estadual Paulista (Unesp)
Resumen
This study evaluated the cohesive strength of composite using self-etching adhesive systems (SE) in the lubrication of instruments between layers of composite. The specimens were made by using a Teflon (R) device. SE were used at the interface to lubricate the instruments: Group 1(G1) - control group, no lubricant was used; Group 2(G2) -Futurabond (R) M; Group 3(G3) - Optibond (R) All-In-One; Group 4(G4) - Clearfil (R) SE Bond; Group 5(G5) - Futurabond (R) NR; Group 6(G6) - Adper (R) SE Plus; Group 7(G7) - One Up Bond (R) F. Specimens were submitted to the tensile test to evaluate the cohesive strength. Data were submitted to the ANOVA and Tukey tests. ANOVA showed a value of p = 0.00. The average means (SD): G2 = 11.33(+/-3.44) a, G3 = 15.36(+/-4.06) ab, G4 = 18.9(+/-4.72) bc, G7 = 19.62(+/-4.46) bc, G5 = 21.02(+/-5.09) bc, G6 = 23.39(+/-4.17) cd, and G1 = 28.49(+/-2.89) d. All SE decreased the cohesive strength of the composite, except for Adper (R) SE Plus.