Microtensile bond strength of different adhesive systems in dentin irradiated with Er : YAG laser
Fecha
2008-07-01Registro en:
Laser Physics Letters. Weinheim: Wiley-v C H Verlag Gmbh, v. 5, n. 7, p. 547-551, 2008.
1612-2011
10.1002/lapl.200810031
WOS:000257568000010
Autor
Universidade Estadual Paulista (Unesp)
Universidade de São Paulo (USP)
Resumen
The objective this study was to evaluate in vitro the bond strength of two etch-and-rise and one self-etching adhesive system after dentin irradiation with Er:YAG (erbium: yttrium aluminum garnet) laser using microtensile test. The results revealed that the groups treated with laser Er:YAG presented less tensile bond strength, independently to the adhesive system used. The prompt L-pop adhesive presented less microtensile bond strength compared to the other adhesives evaluated. There was no difference between single bond and excite groups. The adhesive failures were predominant in all the experimental groups. The Er:YAG laser influenced negatively bond strength values of adhesive systems tested in dental substrate.