Buscar
Mostrando ítems 31-40 de 4713
Effect of annealing on the semicrystalline structure of normal and waxy corn starches
(Elsevier B.V., 2012-10-01)
The influence of amylose and amylopectin on structural reorganization occurred during annealing was studied for normal and waxy corn starches. Annealing caused an increase in crystallinity in the waxy corn starch, whereas ...
Grãos ultrafinos por laminação a morno e recozimento intercrítico
(2006-11-01)
Grain refinement of low carbon steel via the warm deformation of martensite during torsion testing was investigated. At the beginning of straining, laths with high dislocation density were observed. After large deformations, ...
a-Si:H crystallization from isothermal annealing and its dependence on the substrate used
(2012-11-27)
We present hydrogenated amorphous silicon ( a-Si:H) films which were deposited on two different sub
strates (glass and mono-crystalline silicon) after an isothermal annealing treatment at 250"( for up to
14 h.The ...
a-Si:H crystallization from isothermal annealing and its dependence on the substrate used
(2012-12-17)
We present hydrogenated amorphous silicon (a-Si:H) films which were deposited on two different substrates
(glass and mono-crystalline silicon) after an isothermal annealing treatment at 250 ◦C for up to
14 h. The annealed ...
a-Si:H crystallization from isothermal annealing and its dependence on the substrate used
(2012-11-27)
We present hydrogenated amorphous silicon (a-Si:H) films which were deposited on two different substrates
(glass and mono-crystalline silicon) after an isothermal annealing treatment at 250 ◦C for up to
14 h. The annealed ...
Grãos ultrafinos por laminação a morno e recozimento intercrítico
(2006-11-01)
Grain refinement of low carbon steel via the warm deformation of martensite during torsion testing was investigated. At the beginning of straining, laths with high dislocation density were observed. After large deformations, ...
a-Si:H crystallization from isothermal annealing and its dependence on the substrate used
(2012-11-27)
We present hydrogenated amorphous silicon ( a-Si:H) films which were deposited on two different sub
strates (glass and mono-crystalline silicon) after an isothermal annealing treatment at 250"( for up to
14 h.The ...
Estudo do annealing de traços de fissão em epídoto
(Universidade Estadual Paulista (Unesp), 2010-12-16)
No presente trabalho foram efetuados estudos sobre o annealing dos traços de fissão em epídoto. Os experimentos foram feitos aquecendo-se o mineral por tempos de 1, 10 e 100 horas, variando a temperatura de 350 a 950°C. ...
Estudo do annealing de traços de fissão em epídoto
(Universidade Estadual Paulista (Unesp), 2010-12-16)
No presente trabalho foram efetuados estudos sobre o annealing dos traços de fissão em epídoto. Os experimentos foram feitos aquecendo-se o mineral por tempos de 1, 10 e 100 horas, variando a temperatura de 350 a 950°C. ...
Effect of annealing conditions on the optical properties and surface morphologies of (201)-oriented β-Ga2O3 crystals
(Elsevier Science, 2021-10)
The bulk properties of β-Ga2O3 are sensitive to temperature and atmosphere; therefore, suitable annealing conditions are required. This study was performed to investigate the effects of annealing conditions on the (201) ...