Buscar
Mostrando ítems 1-10 de 26
Microstructure development during directional solidification of Sn–Ag–Cu ternary alloys
(Maney Publishing, 2018-03)
Replace of Pb–Sn with Pb-free solders (LFS) is one of the most important issues in the electronic industry. Eutectic and near-eutectic Sn–Ag–Cu (SAC) alloys are recommended as lead-free replacement in welding processes of ...
Manufacture of continuous metal matrix composite strip reinforced by particulate materials from the semisolid processing
(2019-01-01)
Strip casting is a new method of producing metal matrix composites. Two-roll melt dragged processing (TRMD-ing) and single-roll melt dragged processing (SRMD-ing) methods were used to study the manufacture of 2-mm-thick ...
Continuous production of metal matrix composites from the semisolid state
(2013-01-01)
Continuous strip metal matrix composite (MMC) casting of 0.3 mm diameter hard-drawn stainless steel (316L) wire in a quasi-eutectic SnPb (64Sn36Pb) matrix was performed by a two-roll melt drag processing (TRMDping) method, ...
Continuous production of metal matrix composites from the semisolid state
(2013-01-01)
Continuous strip metal matrix composite (MMC) casting of 0.3 mm diameter hard-drawn stainless steel (316L) wire in a quasi-eutectic SnPb (64Sn36Pb) matrix was performed by a two-roll melt drag processing (TRMDping) method, ...
Effects Of Electrodiffusion On The Pb-sn Eutectic Growth
(ABEQ, Sao Paulo, Brazil, 1998)
Directional solidification of Sn-Ag-Cu alloys
(Elsevier, 2015-04)
The alloys of Sn-Ag-Cu family (SAC) are candidates for lead-free replacement of Sn-Pb eutectic used in welding processes of electronic devices. These alloys, with eventual adding of Zn, In and Bi highly improves the ...
Experimental investigation of factors affecting surface quality of Al-Cu alloys ingots
(Elsevier Science SaLausanneSuíça, 2006)
Continuous production of a multi-filament reinforced metal matrix composite strip from the semisolid state
(2014-01-01)
Continuous metal matrix composite strip casting (MMCS-ing) composed of six 0.3-mm diameter annealed bare copper wires in a eutectic SnPb matrix was manufactured by a two-roll melt dragged processing (TRMD-ing) method at a ...