SnO 2 ceramics with low electrical resistivity obtained by microwave sintering
(2011-08-01)
The main aim of this study was to develop dense and conducting SnO 2 ceramics without precipitated phases on the grain boundaries, which was verified using field emission scanning microscopy (FE-SEM) coupled with an ...
SnO 2 ceramics with low electrical resistivity obtained by microwave sintering
(2011-08-01)
The main aim of this study was to develop dense and conducting SnO 2 ceramics without precipitated phases on the grain boundaries, which was verified using field emission scanning microscopy (FE-SEM) coupled with an ...
High-pressure assisted sintering of Ti-20Si-10B and Ti-10Si-5B powders
(2012-11-26)
This work presents the structural characterization of Ti-10Si-5B and Ti-20Si-10B (at-%) alloys produced by high-pressure assisted sintering. Sintering was performed in air at 1100 and 1200°C for 60 s using pressure levels ...
High-pressure assisted sintering of Ti-20Si-10B and Ti-10Si-5B powders
(2012-11-26)
This work presents the structural characterization of Ti-10Si-5B and Ti-20Si-10B (at-%) alloys produced by high-pressure assisted sintering. Sintering was performed in air at 1100 and 1200°C for 60 s using pressure levels ...
A case study of ceramic processing: Microstructural development and electrical properties of Ce0.8Gd0.2O1.9
(2020-06-01)
The effects of powder characteristics and conformation methods on green microstructure have been investigated, and microstructural evolution was analyzed based on the green density and the different sintering techniques. ...
High-Pressure Assisted Sintering of Ti-20Si-10B and Ti-10Si-5B Powders
(Trans Tech Publications Ltd, 2012-01-01)
This work presents the structural characterization of Ti-10Si-5B and Ti-20Si-10B (at-%) alloys produced by high-pressure assisted sintering. Sintering was performed in air at 1100 and 1200 degrees C for 60 s using pressure ...
Evolution of the fractal structure during sintering of SnO2 compacted sol-gel powder
(1995-04-28)
The structural evolution during sintering of compacted SnO2 sol-gel powder was investigated using nitrogen adsorption isotherm analysis. Results show that for sintering temperatures up to 400°C the samples have a fractal ...
Evolution of the fractal structure during sintering of SnO2 compacted sol-gel powder
(1995-04-28)
The structural evolution during sintering of compacted SnO2 sol-gel powder was investigated using nitrogen adsorption isotherm analysis. Results show that for sintering temperatures up to 400°C the samples have a fractal ...