Thermal degradation of geomembranes after exposure to heat
(Millpress Science Publishers, 2006-01-01)
HDPE and PVC geomembranes are sensitive to changes in their properties when in contact with high temperatures. The effects of hot temperature on polymeric geomembranes are assessed by the ASTM D794 and ASTM D5721.This paper ...
Evaluation of mechanical and thermal properties after chemical degradation of PVC and HDPE geomembranes
(2013-06-10)
Chemical compatibility between geomembranes and site-specific waste liquids should be assessed since the waste liquids are highly complex mixtures. This paper presents some considerations about the chemical compatibility ...
Influence of the degradation on the stress cracking values of high density polyethylene (HDPE) geomembranes after different exposures
(2012-12-03)
This paper presents results from stress cracking (SC) tests performed in both fresh and exposed high density polyethylene (HDPE) geomembranes (GM). The HDPE GMs were exposed to ultraviolet radiation, thermal aging (air ...
Thermo-gravimetric analysis (TGA) after different exposures of high density polyethylene (HDPE) and poly vinyl chloride (PVC) geomembranes
(2012-12-03)
This paper presents the results of thermogravimetric analysis (TGA) tests in PVC (1.0; 2.0 mm) and HDPE (0.8; 2.5 mm) geomembranes exposed to weathering and leachate after 30 months. The aim of this paper is the comparison ...
Evaluation of geomembrane UV degradation using melt flow index and oxidative induction time tests
(Zhejiang Univ Press, 2008-01-01)
Many factors such as the sunlight, intensity of radiation, temperature, and moisture may influence the degradation process of geosynthetics. UV stabilizers are used especially in polyolefin geomembrane to prevent the ...
The Effects of Weathering Exposure on the Physical, Mechanical, and Thermal Properties of High-density Polyethylene and Poly (Vinyl Chloride)
(Univ Fed Sao Carlos, Dept Engenharia Materials, 2013-11-01)
This paper presents results describing the physical, mechanical, and thermal properties (melt flow index - MFI and oxidative induction time - OIT) of high density polyethylene and poly (vinyl chloride) after weathering ...
Thermal degradation of geomembranes after exposure to heat
(Millpress Science Publishers, 2014)